Final Magnetic Moment1.871 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.250 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.523 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeSe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 276.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 251.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 65.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 46.5 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 92.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 121.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 209.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 118.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 92.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 118.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 64.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 161.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 195.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 118.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 193.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 197.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 250.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 158.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 144.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 37.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 52.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 64.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 64.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 121.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 223.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 105.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 236.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 83.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 118.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 139.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 223.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 176.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 269.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 325.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 121.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 288.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 37.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 52.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 64.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 158.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 144.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 83.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 144.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 112.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 16.1 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 118.4 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 65.8 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 257.9 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 274.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 83.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
193 | 66 | 59 | 0 | 0 | 0 |
66 | 193 | 59 | 0 | 0 | 0 |
59 | 59 | 205 | 0 | 0 | 0 |
0 | 0 | 0 | 55 | 0 | 0 |
0 | 0 | 0 | 0 | 55 | 0 |
0 | 0 | 0 | 0 | 0 | 57 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.1 | -1.7 | -1.3 | 0 | 0 | 0 |
-1.7 | 6.1 | -1.3 | 0 | 0 | 0 |
-1.3 | -1.3 | 5.6 | 0 | 0 | 0 |
0 | 0 | 0 | 18.3 | 0 | 0 |
0 | 0 | 0 | 0 | 18.3 | 0 |
0 | 0 | 0 | 0 | 0 | 17.6 |
Shear Modulus GV60 GPa |
Bulk Modulus KV107 GPa |
Shear Modulus GR60 GPa |
Bulk Modulus KR107 GPa |
Shear Modulus GVRH60 GPa |
Bulk Modulus KVRH107 GPa |
Elastic Anisotropy0.06 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbEuIn2 (mp-977365) | 0.0190 | 1.390 | 3 |
GdInPd2 (mp-624070) | 0.0204 | 1.273 | 3 |
NaEu2Sn (mp-866536) | 0.0155 | 0.154 | 3 |
LiGd2Ir (mp-862765) | 0.0207 | 0.000 | 3 |
MnGaNi2 (mp-1064170) | 0.0189 | 0.008 | 3 |
VFeCoGe (mp-1063914) | 0.0385 | 0.000 | 4 |
TiFeCoAs (mp-998974) | 0.0385 | 0.236 | 4 |
TiGaFeCo (mp-998964) | 0.0385 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0385 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0385 | 0.028 | 4 |
SrSi (mp-6907) | 0.0185 | 0.372 | 2 |
SrH3 (mp-978856) | 0.0187 | 0.347 | 2 |
MnRh (mp-417) | 0.0185 | 0.000 | 2 |
AlFe (mp-985577) | 0.0182 | 0.000 | 2 |
VRu (mp-1395) | 0.0185 | 0.000 | 2 |
Cu (mp-998890) | 0.0385 | 0.037 | 1 |
Kr (mp-974400) | 0.0385 | 0.002 | 1 |
H2 (mp-632250) | 0.0385 | 0.000 | 1 |
Ge (mp-998883) | 0.0385 | 0.340 | 1 |
S (mp-1063988) | 0.0234 | 1.137 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv Se |
Final Energy/Atom-5.7321 eV |
Corrected Energy-11.4642 eV
-11.4642 eV = -11.4642 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)