material

CoSn2

ID:

mp-20155

DOI:

10.17188/1195297


Tags: Cobalt tin (1/2) Cobalt stannide (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.072 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.013 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.84 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoSn3 + CoSn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 102672 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <0 0 1> 0.001 41.0
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.001 175.3
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.001 269.6
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.003 105.2
Al (mp-134) <1 0 0> <0 0 1> 0.012 81.9
MgO (mp-1265) <1 0 0> <0 0 1> 0.015 163.8
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.029 175.3
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.031 163.8
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.033 215.6
LiNbO3 (mp-3731) <1 1 0> <1 1 1> 0.034 128.6
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.042 140.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.042 327.6
CeO2 (mp-20194) <1 0 0> <1 1 0> 0.047 148.8
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.048 81.9
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.051 210.4
Si (mp-149) <1 0 0> <1 1 0> 0.051 148.8
Mg (mp-153) <0 0 1> <1 0 0> 0.051 35.1
InP (mp-20351) <1 1 1> <1 0 0> 0.052 245.4
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.054 140.3
Si (mp-149) <1 1 0> <1 0 0> 0.054 210.4
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.056 347.1
GaAs (mp-2534) <1 0 0> <0 0 1> 0.063 163.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.072 35.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.072 327.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.073 35.1
GaSe (mp-1943) <1 0 0> <1 0 1> 0.078 269.6
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.086 175.3
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.087 35.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.091 163.8
WS2 (mp-224) <1 1 1> <1 0 0> 0.100 315.6
KCl (mp-23193) <1 1 0> <1 0 0> 0.102 175.3
Cu (mp-30) <1 0 0> <1 1 0> 0.112 198.3
Cu (mp-30) <1 1 0> <1 0 0> 0.112 280.5
LaF3 (mp-905) <1 1 0> <1 0 0> 0.112 280.5
WS2 (mp-224) <1 0 0> <1 0 1> 0.119 269.6
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.134 269.6
Ge (mp-32) <1 0 0> <0 0 1> 0.137 163.8
SiC (mp-11714) <1 0 0> <1 1 0> 0.141 247.9
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.142 280.5
C (mp-66) <1 0 0> <0 0 1> 0.144 163.8
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.145 247.9
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.164 215.6
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.165 215.6
InSb (mp-20012) <1 1 0> <1 0 0> 0.167 315.6
Au (mp-81) <1 1 0> <1 0 0> 0.180 245.4
Ag (mp-124) <1 1 0> <1 0 0> 0.180 245.4
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.182 140.3
CdTe (mp-406) <1 1 0> <1 0 0> 0.193 315.6
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.199 161.7
CdS (mp-672) <1 0 0> <1 1 0> 0.207 198.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
182 57 57 0 0 0
57 200 50 0 0 0
57 50 200 0 0 0
0 0 0 63 0 0
0 0 0 0 40 0
0 0 0 0 0 40
Compliance Tensor Sij (10-12Pa-1)
6.4 -1.5 -1.5 0 0 0
-1.5 5.7 -1 0 0 0
-1.5 -1 5.7 0 0 0
0 0 0 15.9 0 0
0 0 0 0 24.8 0
0 0 0 0 0 24.8
Shear Modulus GV
56 GPa
Bulk Modulus KV
101 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
101 GPa
Shear Modulus GVRH
55 GPa
Bulk Modulus KVRH
101 GPa
Elastic Anisotropy
0.34
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.2094 0.044 3
Ta4FeP (mp-22444) 0.1988 0.055 3
Nb4FeSi (mp-22312) 0.3058 0.048 3
Nb4CoSi (mp-10003) 0.3486 0.013 3
Zr4CuP (mp-581733) 0.3135 0.063 3
Co2B (mp-1071320) 0.0680 0.079 2
Co2B (mp-493) 0.0728 0.079 2
Tl2Pd (mp-570896) 0.0317 0.000 2
Zr2Rh (mp-571664) 0.0720 0.000 2
BMo2 (mp-2501) 0.0902 0.018 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Co Sn_d
Final Energy/Atom
-5.1027 eV
Corrected Energy
-30.6159 eV
Uncorrected energy = -30.6159 eV Corrected energy = -30.6159 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 102672
  • 247484
  • 625269
  • 625263
  • 409910
  • 625260
  • 108319
Submitted by
User remarks:
  • Cobalt tin (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)