material

MnCoP

ID:

mp-20249

DOI:

10.17188/1195381


Tags: Cobalt manganese phosphide (1/1/1) - HT Cobalt manganese phosphide (1/1/1)

Material Details

Final Magnetic Moment
2.999 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.643 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.10 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 41556 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Fe2O3 (mp-24972) <1 1 0> <0 1 1> 0.000 123.2
LiTaO3 (mp-3666) <1 0 1> <0 0 1> 0.016 305.2
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.028 115.6
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.028 115.6
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.030 223.8
YAlO3 (mp-3792) <1 1 1> <1 1 1> 0.035 249.7
ZnO (mp-2133) <1 1 1> <0 1 0> 0.040 254.3
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.042 299.6
C (mp-48) <0 0 1> <1 1 1> 0.047 99.9
BaF2 (mp-1029) <1 1 0> <0 1 1> 0.077 277.2
MoSe2 (mp-1634) <1 0 1> <0 1 0> 0.085 208.1
TiO2 (mp-2657) <1 0 0> <0 1 1> 0.088 123.2
TiO2 (mp-390) <1 0 0> <0 0 1> 0.088 183.1
SiC (mp-11714) <0 0 1> <1 0 0> 0.109 157.2
GaP (mp-2490) <1 1 1> <1 0 0> 0.110 157.2
C (mp-48) <1 1 0> <1 0 0> 0.112 235.8
KP(HO2)2 (mp-23959) <1 0 0> <1 1 0> 0.113 228.0
SiC (mp-7631) <0 0 1> <1 0 0> 0.113 157.2
Fe2O3 (mp-24972) <0 0 1> <0 1 1> 0.113 92.4
Te2W (mp-22693) <0 0 1> <0 1 1> 0.114 154.0
SiC (mp-8062) <1 1 1> <0 0 1> 0.115 264.5
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.116 138.7
MoSe2 (mp-1634) <1 0 0> <0 1 0> 0.120 208.1
Te2W (mp-22693) <0 1 1> <0 1 0> 0.124 115.6
GaP (mp-2490) <1 1 0> <0 1 0> 0.135 300.5
CaF2 (mp-2741) <1 1 1> <1 0 0> 0.143 157.2
CaF2 (mp-2741) <1 1 0> <0 1 0> 0.144 300.5
LiGaO2 (mp-5854) <1 1 0> <0 1 1> 0.150 338.8
Te2W (mp-22693) <0 1 0> <0 1 0> 0.161 161.8
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.162 299.6
WS2 (mp-224) <1 0 0> <1 0 0> 0.164 314.5
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.165 117.9
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.168 183.1
BaF2 (mp-1029) <1 1 1> <0 1 1> 0.168 277.2
CdWO4 (mp-19387) <0 1 1> <0 1 0> 0.171 161.8
Si (mp-149) <1 1 1> <1 0 0> 0.174 157.2
Ni (mp-23) <1 0 0> <0 0 1> 0.175 61.0
CeO2 (mp-20194) <1 1 1> <1 0 0> 0.182 157.2
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.185 244.2
LiNbO3 (mp-3731) <1 0 1> <0 0 1> 0.186 305.2
Cu (mp-30) <1 1 0> <1 1 1> 0.207 149.8
Ni (mp-23) <1 1 0> <0 1 0> 0.210 69.4
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.218 273.6
KTaO3 (mp-3614) <1 1 1> <0 1 0> 0.218 369.9
Au (mp-81) <1 1 1> <0 0 1> 0.226 61.0
AlN (mp-661) <1 1 1> <1 0 0> 0.226 196.5
AlN (mp-661) <1 0 0> <1 0 1> 0.233 221.3
ZrO2 (mp-2858) <0 0 1> <1 0 1> 0.237 221.3
CdTe (mp-406) <1 1 0> <0 1 0> 0.245 185.0
InP (mp-20351) <1 0 0> <0 0 1> 0.250 142.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
290 121 138 0 0 0
121 385 148 0 0 0
138 148 312 0 0 0
0 0 0 122 0 0
0 0 0 0 117 0
0 0 0 0 0 111
Compliance Tensor Sij (10-12Pa-1)
4.6 -0.8 -1.6 0 0 0
-0.8 3.3 -1.2 0 0 0
-1.6 -1.2 4.5 0 0 0
0 0 0 8.2 0 0
0 0 0 0 8.5 0
0 0 0 0 0 9
Shear Modulus GV
109 GPa
Bulk Modulus KV
200 GPa
Shear Modulus GR
106 GPa
Bulk Modulus KR
197 GPa
Shear Modulus GVRH
107 GPa
Bulk Modulus KVRH
199 GPa
Elastic Anisotropy
0.14
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TaSiRh (mp-20436) 0.1521 0.000 3
NbSiPt (mp-10469) 0.1410 0.000 3
NbSiPd (mp-22722) 0.1537 0.000 3
VSiNi (mp-1095532) 0.1363 0.000 3
Na2LiGaAs2 (mp-9722) 0.3981 0.000 4
Na2LiAlP2 (mp-9719) 0.4525 0.000 4
K2LiInAs2 (mp-505431) 0.3746 0.000 4
K3Na2SnBi3 (mp-568329) 0.4417 0.000 4
K2NaInSb2 (mp-505767) 0.4952 0.000 4
ThSe2 (mp-7951) 0.4765 0.000 2
YbH2 (mp-864603) 0.4592 0.000 2
CaH2 (mp-23713) 0.4508 0.000 2
SrH2 (mp-23714) 0.4537 0.000 2
BaH2 (mp-23715) 0.4619 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Co P
Final Energy/Atom
-7.8704 eV
Corrected Energy
-94.4449 eV
Uncorrected energy = -94.4449 eV Corrected energy = -94.4449 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 16483
  • 41557
  • 41556
  • 106483
Submitted by
User remarks:
  • Cobalt manganese phosphide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)