material

NbInSe2

ID:

mp-20279

DOI:

10.17188/1195409


Tags: Indium niobium selenide (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.690 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.22 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6m2 [187]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.000 124.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.001 124.7
Al (mp-134) <1 1 1> <0 0 1> 0.001 197.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.004 197.5
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.004 197.5
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.007 281.8
InAs (mp-20305) <1 1 1> <0 0 1> 0.014 197.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.020 31.2
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.020 197.5
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.028 292.8
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.029 292.8
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.029 307.4
ZnO (mp-2133) <1 0 1> <1 0 1> 0.034 239.1
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.035 218.3
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.038 332.7
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.040 343.0
InP (mp-20351) <1 0 0> <0 0 1> 0.041 249.5
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.043 155.9
MgO (mp-1265) <1 0 0> <0 0 1> 0.043 197.5
LaF3 (mp-905) <0 0 1> <0 0 1> 0.046 135.1
LiTaO3 (mp-3666) <1 0 1> <1 0 1> 0.052 307.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.060 218.3
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.062 124.7
Mg (mp-153) <1 0 1> <1 0 1> 0.064 170.8
Ni (mp-23) <1 1 1> <1 0 1> 0.064 170.8
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.069 155.9
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.070 249.5
NaCl (mp-22862) <1 1 1> <0 0 1> 0.074 166.3
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.076 292.8
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.083 281.8
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.083 280.7
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.084 259.9
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.086 357.9
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.088 135.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.095 249.5
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.101 280.7
BN (mp-984) <1 0 1> <0 0 1> 0.102 218.3
MoS2 (mp-1434) <1 1 0> <1 0 1> 0.102 239.1
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.105 291.1
AlN (mp-661) <1 0 0> <1 0 1> 0.115 239.1
SiC (mp-11714) <1 0 1> <0 0 1> 0.120 259.9
CdSe (mp-2691) <1 1 1> <0 0 1> 0.121 197.5
Al (mp-134) <1 1 0> <0 0 1> 0.123 207.9
SiC (mp-7631) <1 0 0> <1 0 1> 0.133 239.1
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.135 207.9
SiC (mp-8062) <1 1 1> <0 0 1> 0.141 135.1
KCl (mp-23193) <1 1 0> <0 0 1> 0.142 291.1
TiO2 (mp-390) <1 1 1> <0 0 1> 0.142 218.3
InP (mp-20351) <1 1 0> <0 0 1> 0.142 249.5
TiO2 (mp-390) <1 0 1> <1 0 0> 0.148 195.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
105 28 11 0 0 0
28 105 11 0 0 0
11 11 88 0 0 0
0 0 0 6 0 0
0 0 0 0 6 0
0 0 0 0 0 39
Compliance Tensor Sij (10-12Pa-1)
10.3 -2.6 -1 0 0 0
-2.6 10.3 -1 0 0 0
-1 -1 11.6 0 0 0
0 0 0 163.6 0 0
0 0 0 0 163.6 0
0 0 0 0 0 25.8
Shear Modulus GV
27 GPa
Bulk Modulus KV
45 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
44 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
44 GPa
Elastic Anisotropy
5.77
Poisson's Ratio
0.31

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
42
U Values
--
Pseudopotentials
VASP PAW: Se Nb_pv In_d
Final Energy/Atom
-5.6446 eV
Corrected Energy
-22.5784 eV
-22.5784 eV = -22.5784 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53102

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)