Final Magnetic Moment0.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.397 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
CdS (mp-672) | <1 1 1> | <1 1 1> | 0.003 | 156.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 0.004 | 187.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 0.006 | 25.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 0.011 | 128.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 0.015 | 176.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 0.024 | 125.1 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 0.027 | 230.5 |
WS2 (mp-224) | <1 1 1> | <1 1 0> | 0.030 | 235.9 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 0.031 | 179.3 |
ZnO (mp-2133) | <0 0 1> | <1 1 0> | 0.041 | 176.9 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 0.041 | 59.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 0.057 | 83.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 0.057 | 83.4 |
WS2 (mp-224) | <1 1 0> | <1 1 0> | 0.057 | 235.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 0.070 | 128.1 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 0.072 | 88.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 0.080 | 83.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 0.084 | 230.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 0.113 | 231.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 0.114 | 83.4 |
GaTe (mp-542812) | <1 0 1> | <1 0 0> | 0.115 | 291.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 0.122 | 83.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 0.125 | 117.9 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 0.146 | 128.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 0.148 | 187.6 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 0.149 | 166.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 0.151 | 33.0 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 0.166 | 179.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 0.168 | 128.1 |
MoSe2 (mp-1634) | <1 1 1> | <1 0 0> | 0.173 | 271.0 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 0.176 | 333.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 0.192 | 125.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 0.195 | 230.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 0.197 | 62.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 0.197 | 187.6 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 0.199 | 229.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 0.207 | 179.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 0.237 | 179.3 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 0.245 | 59.0 |
GaTe (mp-542812) | <1 0 0> | <1 1 0> | 0.248 | 88.5 |
TiO2 (mp-390) | <0 0 1> | <1 1 1> | 0.255 | 117.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 0.256 | 294.9 |
Si (mp-149) | <1 1 0> | <1 1 0> | 0.260 | 294.9 |
SiC (mp-11714) | <0 0 1> | <1 1 0> | 0.263 | 59.0 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 0.268 | 294.9 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 0.270 | 273.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 0.276 | 76.8 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 0.277 | 235.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 1> | 0.287 | 198.2 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 0> | 0.297 | 59.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
489 | 214 | 214 | 0 | 0 | 0 |
214 | 532 | 237 | 0 | 0 | 0 |
214 | 237 | 532 | 0 | 0 | 0 |
0 | 0 | 0 | 163 | 0 | 0 |
0 | 0 | 0 | 0 | 214 | 0 |
0 | 0 | 0 | 0 | 0 | 214 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2.7 | -0.8 | -0.8 | 0 | 0 | 0 |
-0.8 | 2.6 | -0.8 | 0 | 0 | 0 |
-0.8 | -0.8 | 2.6 | 0 | 0 | 0 |
0 | 0 | 0 | 6.1 | 0 | 0 |
0 | 0 | 0 | 0 | 4.7 | 0 |
0 | 0 | 0 | 0 | 0 | 4.7 |
Shear Modulus GV177 GPa |
Bulk Modulus KV320 GPa |
Shear Modulus GR172 GPa |
Bulk Modulus KR319 GPa |
Shear Modulus GVRH175 GPa |
Bulk Modulus KVRH320 GPa |
Elastic Anisotropy0.15 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb4CoP (mp-21447) | 0.1741 | 0.044 | 3 |
Nb4SiNi (mp-22396) | 0.1690 | 0.009 | 3 |
Ta4FeP (mp-22444) | 0.2776 | 0.055 | 3 |
Nb4CoSi (mp-10003) | 0.2718 | 0.013 | 3 |
Zr4CuP (mp-581733) | 0.1690 | 0.063 | 3 |
Ta2Be (mp-11278) | 0.0762 | 0.000 | 2 |
Tl2Pt (mp-571160) | 0.0784 | 0.006 | 2 |
Pb2Au (mp-22795) | 0.0606 | 0.000 | 2 |
Zr2Si (mp-1278) | 0.0416 | 0.000 | 2 |
Th2Au (mp-1629) | 0.0498 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv B |
Final Energy/Atom-8.7314 eV |
Corrected Energy-52.3884 eV
-52.3884 eV = -52.3884 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)