MnNbP

ID:

mp-20335

DOI:

10.17188/1195457


Tags: Niobium manganese phosphide (1/1/1)

Material Details

Final Magnetic Moment
0.009 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.786 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.46 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 68280 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <0 1 0> 0.002 231.6
SiC (mp-11714) <1 1 0> <0 1 1> 0.005 271.9
KCl (mp-23193) <1 0 0> <1 1 0> 0.011 205.1
GdScO3 (mp-5690) <1 1 0> <0 1 0> 0.011 128.6
SiC (mp-8062) <1 1 1> <0 0 1> 0.012 66.6
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.016 288.6
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.017 128.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.019 66.6
ZnO (mp-2133) <0 0 1> <1 0 0> 0.020 177.4
SiC (mp-11714) <0 0 1> <0 0 1> 0.024 66.6
CaCO3 (mp-3953) <1 0 1> <0 1 0> 0.028 180.1
SiC (mp-7631) <1 0 1> <0 1 0> 0.045 334.5
C (mp-66) <1 0 0> <0 1 0> 0.049 25.7
NaCl (mp-22862) <1 0 0> <0 1 0> 0.059 128.6
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.059 199.8
PbSe (mp-2201) <1 0 0> <0 0 1> 0.067 155.4
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.068 244.2
Cu (mp-30) <1 1 0> <0 0 1> 0.070 111.0
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.072 99.2
CdS (mp-672) <1 0 0> <0 1 0> 0.075 231.6
GaN (mp-804) <0 0 1> <0 1 0> 0.076 180.1
GaSb (mp-1156) <1 0 0> <0 0 1> 0.080 155.4
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.086 244.2
LaAlO3 (mp-2920) <0 0 1> <0 1 1> 0.089 101.9
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.091 256.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.101 155.4
C (mp-48) <1 0 1> <1 0 1> 0.117 99.2
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.119 128.6
WS2 (mp-224) <1 0 0> <0 1 1> 0.123 135.9
Te2W (mp-22693) <1 1 0> <1 0 0> 0.125 221.7
KP(HO2)2 (mp-23959) <0 1 0> <0 1 0> 0.126 77.2
Au (mp-81) <1 1 0> <1 0 0> 0.146 221.7
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.150 111.0
TbScO3 (mp-31119) <1 1 0> <0 1 0> 0.162 128.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.164 22.2
KP(HO2)2 (mp-23959) <1 0 0> <0 1 0> 0.168 231.6
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.169 155.4
MgO (mp-1265) <1 1 1> <0 1 0> 0.183 283.0
Ag (mp-124) <1 1 0> <1 0 0> 0.188 221.7
LaAlO3 (mp-2920) <1 0 1> <0 1 1> 0.198 305.8
TiO2 (mp-390) <1 0 1> <0 0 1> 0.208 199.8
DyScO3 (mp-31120) <0 0 1> <0 1 0> 0.209 283.0
GaN (mp-804) <1 0 1> <1 0 0> 0.211 133.0
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.215 283.0
SiC (mp-8062) <1 0 0> <0 0 1> 0.224 155.4
Al (mp-134) <1 0 0> <0 1 0> 0.228 128.6
BaTiO3 (mp-5986) <1 1 1> <1 0 1> 0.247 198.4
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.251 111.0
BN (mp-984) <1 0 1> <0 1 0> 0.266 180.1
CdS (mp-672) <1 1 1> <0 1 0> 0.280 51.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
371 111 211 0 0 0
111 344 190 0 0 0
211 190 324 0 0 0
0 0 0 141 0 0
0 0 0 0 118 0
0 0 0 0 0 95
Compliance Tensor Sij (10-12Pa-1)
4.3 0.2 -2.9 0 0 0
0.2 4.3 -2.7 0 0 0
-2.9 -2.7 6.6 0 0 0
0 0 0 7.1 0 0
0 0 0 0 8.4 0
0 0 0 0 0 10.5
Shear Modulus GV
106 GPa
Bulk Modulus KV
229 GPa
Shear Modulus GR
94 GPa
Bulk Modulus KR
227 GPa
Shear Modulus GVRH
100 GPa
Bulk Modulus KVRH
228 GPa
Elastic Anisotropy
0.68
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CoBMo (mp-21347) 0.2001 0.000 3
CaInPd (mp-620571) 0.1951 0.000 3
CoBW (mp-22759) 0.1617 0.000 3
CoReB (mp-21464) 0.1792 0.009 3
NbSiRh (mp-10470) 0.2131 0.000 3
Na2LiGaAs2 (mp-9722) 0.5260 0.000 4
Na2LiAlP2 (mp-9719) 0.5686 0.000 4
K2LiInAs2 (mp-505431) 0.5140 0.000 4
K3Na2SnBi3 (mp-568329) 0.5541 0.000 4
K2NaInSb2 (mp-505767) 0.5956 0.000 4
US2 (mp-639) 0.5665 0.000 2
YbH2 (mp-864603) 0.5077 0.000 2
CaH2 (mp-23713) 0.5291 0.000 2
SrH2 (mp-23714) 0.5209 0.000 2
BaH2 (mp-23715) 0.5057 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Nb_pv P
Final Energy/Atom
-9.0111 eV
Corrected Energy
-108.1331 eV
-108.1331 eV = -108.1331 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 68280
Submitted by
User remarks:
  • Niobium manganese phosphide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)