Final Magnetic Moment0.011 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.318 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 182.6 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 137.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 79.1 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 228.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 111.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 298.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 237.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 335.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 131.8 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 319.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 111.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 290.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 131.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 290.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 111.8 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 319.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 131.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 111.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 290.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 335.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 274.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 210.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 111.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 186.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 131.8 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 228.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 111.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 131.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 131.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 45.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 261.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 149.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 237.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 74.6 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 158.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 131.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 74.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 149.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 105.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 263.6 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 261.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 290.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 237.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 342.7 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 111.8 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 228.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 52.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 186.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 210.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 26.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
121 | 37 | 37 | 0 | 0 | 0 |
37 | 121 | 37 | 0 | 0 | 0 |
37 | 37 | 121 | 0 | 0 | 0 |
0 | 0 | 0 | 43 | 0 | 0 |
0 | 0 | 0 | 0 | 43 | 0 |
0 | 0 | 0 | 0 | 0 | 43 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.6 | -2.2 | -2.2 | 0 | 0 | 0 |
-2.2 | 9.6 | -2.2 | 0 | 0 | 0 |
-2.2 | -2.2 | 9.6 | 0 | 0 | 0 |
0 | 0 | 0 | 23.4 | 0 | 0 |
0 | 0 | 0 | 0 | 23.4 | 0 |
0 | 0 | 0 | 0 | 0 | 23.4 |
Shear Modulus GV43 GPa |
Bulk Modulus KV65 GPa |
Shear Modulus GR43 GPa |
Bulk Modulus KR65 GPa |
Shear Modulus GVRH43 GPa |
Bulk Modulus KVRH65 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsCdCl3 (mp-568544) | 0.0000 | 0.007 | 3 |
HgIrO3 (mp-1016831) | 0.0000 | 0.402 | 3 |
Ce3AlC (mp-10036) | 0.0000 | 0.000 | 3 |
Dy3AlC (mp-29676) | 0.0000 | 0.000 | 3 |
AlFe3C (mp-22793) | 0.0000 | 0.000 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.749 | 4 |
Ca3Sb2 (mp-1013546) | 0.0000 | 0.421 | 2 |
Ca3Bi2 (mp-1013735) | 0.0000 | 0.366 | 2 |
Mn4N (mp-505622) | 0.0000 | 0.000 | 2 |
Ba3N2 (mp-1013528) | 0.0000 | 0.683 | 2 |
Ca3N2 (mp-1013524) | 0.0000 | 0.512 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.247 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 In_d C |
Final Energy/Atom-5.5742 eV |
Corrected Energy-27.8709 eV
Uncorrected energy = -27.8709 eV
Corrected energy = -27.8709 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)