Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.116 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToInAs |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPa3 [205] |
Hall-P 2ac 2ab 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiC (mp-8062) | <1 1 0> | <1 1 0> | 81.0 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 99.2 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 229.0 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 57.2 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 286.2 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 81.0 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 286.2 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 242.9 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 171.7 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 242.9 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 161.9 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 286.2 |
Cu (mp-30) | <1 0 0> | <1 1 1> | 198.3 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 297.5 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 286.2 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 0> | 242.9 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 286.2 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 297.5 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 161.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 286.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 297.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 242.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 171.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 57.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 81.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 286.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 171.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 297.5 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 242.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 286.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 242.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 297.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 242.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 171.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 286.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 286.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 286.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 198.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 229.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 242.9 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 297.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 99.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 161.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 229.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 171.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 286.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2CrO3 (mp-770149) | 0.7415 | 0.072 | 3 |
CaSnN2 (mp-1029633) | 0.7494 | 0.000 | 3 |
Mg2CrN3 (mp-1029520) | 0.6878 | 0.000 | 3 |
Mg2MnN3 (mp-1029288) | 0.6661 | 0.071 | 3 |
Li5MnOF5 (mp-764320) | 0.7499 | 0.061 | 4 |
GaP (mp-971632) | 0.0749 | 0.172 | 2 |
AlAs (mp-988945) | 0.0696 | 0.151 | 2 |
LaN (mp-567290) | 0.5710 | 0.000 | 2 |
GaAs (mp-15619) | 0.0602 | 0.147 | 2 |
AlSb (mp-15621) | 0.0091 | 0.117 | 2 |
Si (mp-571520) | 0.4387 | 0.161 | 1 |
Ge (mp-128) | 0.5093 | 0.148 | 1 |
C (mp-24) | 0.5386 | 0.833 | 1 |
Si (mp-168) | 0.3261 | 0.160 | 1 |
Ge (mp-1080106) | 0.3256 | 0.146 | 1 |
Explore more synthesis descriptions for materials of composition InAs.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d As |
Final Energy/Atom-3.8215 eV |
Corrected Energy-61.1434 eV
-61.1434 eV = -61.1434 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)