Final Magnetic Moment16.391 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.617 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6 [174] |
HallP 6 |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 90.2 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 0 0> | 260.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 312.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 260.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 312.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 208.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 312.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 260.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 208.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 312.3 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 260.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 208.2 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 208.2 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 104.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 133.6 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 90.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 180.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 260.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 312.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 260.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 312.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 260.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 133.6 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 104.1 |
PbS (mp-21276) | <1 1 1> | <1 1 0> | 180.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 156.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 104.1 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 180.3 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 312.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 312.3 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 104.1 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 260.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 156.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 156.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 270.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 208.2 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 312.3 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 260.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 260.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 156.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 1> | 143.4 |
Ga2O3 (mp-886) | <1 1 -1> | <1 0 0> | 156.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 156.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 52.1 |
Au (mp-81) | <1 1 0> | <1 1 0> | 270.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 156.2 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 312.3 |
C (mp-48) | <1 1 0> | <1 0 0> | 260.3 |
C (mp-48) | <1 1 1> | <1 0 0> | 260.3 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ta2Se8I (mp-30531) | 0.7295 | 0.000 | 3 |
K4Hf3Te17 (mp-581963) | 0.7160 | 0.000 | 3 |
Tb6PbSe10 (mp-675130) | 0.7294 | 0.040 | 3 |
Zr2Cr30P19 (mp-15746) | 0.7000 | 0.016 | 3 |
Th7Te12 (mp-9521) | 0.1943 | 0.000 | 2 |
V12P7 (mp-684675) | 0.3889 | 0.000 | 2 |
Cr2P (mp-29184) | 0.6978 | 0.030 | 2 |
Cr12P7 (mp-505626) | 0.4805 | 0.030 | 2 |
MgGa2 (mp-567539) | 0.6386 | 0.017 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Te |
Final Energy/Atom-6.7623 eV |
Corrected Energy-128.4833 eV
-128.4833 eV = -128.4833 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)