Final Magnetic Moment0.432 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.426 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 337.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 274.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 337.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 168.9 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 243.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 316.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 147.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 274.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 63.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 295.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 211.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 211.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 105.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 337.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 168.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 337.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 274.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 63.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 232.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 337.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 84.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 337.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 316.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 190.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 274.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 105.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 147.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 147.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 147.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 274.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 147.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 274.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 84.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 147.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 232.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 274.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 274.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 63.3 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 274.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 63.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 337.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 337.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 274.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 84.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 190.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 253.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbAl2Cu (mp-977428) | 0.3401 | 0.000 | 3 |
Gd3Al7Ag2 (mp-637182) | 0.3081 | 0.000 | 3 |
GdMg2Ni9 (mp-567249) | 0.3454 | 0.451 | 3 |
CaMg2Ni9 (mp-12695) | 0.3191 | 0.013 | 3 |
Ca3Al7Ag2 (mp-11430) | 0.2872 | 0.000 | 3 |
YNi3 (mp-569196) | 0.0354 | 0.000 | 2 |
ErNi3 (mp-1095554) | 0.0311 | 0.000 | 2 |
YIr3 (mp-1095497) | 0.0678 | 0.020 | 2 |
ErNi3 (mp-1051) | 0.0129 | 0.000 | 2 |
SmNi3 (mp-1095619) | 0.0728 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Ni_pv |
Final Energy/Atom-5.9062 eV |
Corrected Energy-70.8745 eV
-70.8745 eV = -70.8745 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)