material

MnCu2GeS4

ID:

mp-20474

DOI:

10.17188/1195603


Tags: Dicopper manganese tetrathiogermanate Dicopper(I) manganese tetrathiogermanate

Material Details

Final Magnetic Moment
5.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.651 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.265 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmn21 [31]
Hall
P 2ac 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 0 0> <1 0 0> 0.006 148.2
AlN (mp-661) <0 0 1> <0 0 1> 0.006 202.9
SiC (mp-8062) <1 0 0> <1 0 1> 0.009 191.8
AlN (mp-661) <1 0 1> <0 1 0> 0.009 142.1
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.019 273.8
AlN (mp-661) <1 0 0> <0 1 1> 0.020 62.4
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.020 197.6
Al (mp-134) <1 1 1> <1 0 0> 0.020 197.6
TiO2 (mp-390) <1 0 1> <0 1 0> 0.024 236.9
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.024 197.6
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 0 0> 0.025 197.6
C (mp-48) <0 0 1> <1 0 0> 0.027 148.2
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.030 319.6
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.031 98.8
InAs (mp-20305) <1 1 1> <1 0 0> 0.032 197.6
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.037 197.6
ZnTe (mp-2176) <1 1 1> <1 0 0> 0.037 197.6
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.044 197.6
BaF2 (mp-1029) <1 0 0> <0 1 0> 0.045 236.9
LiGaO2 (mp-5854) <0 0 1> <0 1 0> 0.049 331.6
C (mp-66) <1 1 1> <1 0 0> 0.052 197.6
CdS (mp-672) <0 0 1> <1 0 0> 0.053 197.6
BN (mp-984) <0 0 1> <0 0 1> 0.056 81.2
Cu (mp-30) <1 0 0> <1 1 0> 0.060 273.8
SiC (mp-7631) <0 0 1> <0 1 0> 0.063 331.6
SiC (mp-11714) <0 0 1> <0 1 0> 0.063 331.6
TePb (mp-19717) <1 1 0> <0 0 1> 0.066 121.8
C (mp-66) <1 1 0> <0 0 1> 0.067 162.3
SiC (mp-8062) <1 1 0> <0 0 1> 0.067 81.2
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.067 162.3
InAs (mp-20305) <1 1 0> <0 0 1> 0.070 162.3
TePb (mp-19717) <1 0 0> <1 0 1> 0.073 127.9
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.075 202.9
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.076 345.7
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.081 318.3
DyScO3 (mp-31120) <1 1 0> <1 1 1> 0.081 318.3
ZnO (mp-2133) <0 0 1> <1 0 0> 0.085 148.2
TbScO3 (mp-31119) <0 1 1> <1 0 1> 0.086 319.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.095 162.3
SiC (mp-7631) <1 0 0> <0 1 1> 0.097 187.2
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.099 273.8
SiC (mp-11714) <1 0 0> <0 1 1> 0.104 62.4
GaSb (mp-1156) <1 1 0> <0 0 1> 0.112 162.3
CaCO3 (mp-3953) <1 0 1> <1 1 0> 0.112 273.8
Ag (mp-124) <1 0 0> <1 0 1> 0.120 255.7
Te2Mo (mp-602) <1 1 0> <0 1 0> 0.122 94.8
MoSe2 (mp-1634) <1 0 1> <1 1 1> 0.125 159.1
ZnO (mp-2133) <1 0 0> <0 1 0> 0.127 189.5
GaN (mp-804) <1 1 0> <0 0 1> 0.128 324.7
CdSe (mp-2691) <1 1 1> <1 0 0> 0.130 197.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
105 52 44 0 0 0
52 111 45 0 0 0
44 45 133 0 0 0
0 0 0 23 0 0
0 0 0 0 24 0
0 0 0 0 0 24
Compliance Tensor Sij (10-12Pa-1)
13.2 -5.1 -2.7 0 0 0
-5.1 12.4 -2.5 0 0 0
-2.7 -2.5 9.3 0 0 0
0 0 0 43.9 0 0
0 0 0 0 41.6 0
0 0 0 0 0 40.9
Shear Modulus GV
28 GPa
Bulk Modulus KV
70 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
70 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
70 GPa
Elastic Anisotropy
0.25
Poisson's Ratio
0.33

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.04793 0.00000
0.00000 0.00000 0.00000 0.02546 0.00000 0.00000
0.11900 0.13193 -0.20804 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.27358 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
9.53 0.00 0.00
0.00 8.81 0.00
0.00 0.00 10.06
Dielectric Tensor εij (total)
11.06 0.00 0.00
0.00 11.04 0.00
0.00 0.00 12.36
Polycrystalline dielectric constant εpoly
(electronic contribution)
9.47
Polycrystalline dielectric constant εpoly
(total)
11.49
Refractive Index n
3.08
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cu3PSe4 (mp-5756) 0.0988 0.000 3
Li3SbS4 (mp-756316) 0.1573 0.000 3
Cu3SbSe4 (mp-9814) 0.1778 0.000 3
Cu3SbS4 (mp-22171) 0.1318 0.009 3
Cu2SiS3 (mp-561468) 0.1555 0.135 3
ZnCu2SiS4 (mp-977414) 0.1351 0.002 4
CoCu2SnS4 (mp-11770) 0.1759 0.053 4
CoCu2SnS4 (mp-556504) 0.1754 0.053 4
Ag2SnHgSe4 (mp-10963) 0.0700 0.000 4
FeCu2SnS4 (mp-22648) 0.1673 0.039 4
CdTe (mp-685146) 0.2307 0.009 2
CuI (mp-673245) 0.2138 0.008 2
FeO (mp-781777) 0.2238 0.463 2
BC7 (mp-1080030) 0.2317 0.249 2
BC5 (mp-1095514) 0.1773 0.302 2
Sn (mp-949028) 0.2121 0.030 1
Si (mp-971662) 0.2109 0.064 1
C (mp-569517) 0.3034 0.145 1
C (mp-611426) 0.2968 0.146 1
Ge (mp-1091415) 0.2927 0.014 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Cu_pv Ge_d S
Final Energy/Atom
-5.2156 eV
Corrected Energy
-87.4732 eV
Uncorrected energy = -83.4492 eV Composition-based energy adjustment (-0.503 eV/atom x 8.0 atoms) = -4.0240 eV Corrected energy = -87.4732 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 193988
  • 627735
  • 42490
  • 627738
  • 415453
Submitted by
User remarks:
  • Dicopper manganese tetrathiogermanate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)