Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.893 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypePlane
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 240.7 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 178.0 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 222.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 156.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 218.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 249.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 255.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 281.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 255.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 240.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 190.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 255.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 218.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 218.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 221.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 249.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 187.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 281.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 204.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 281.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 222.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.4 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 267.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 255.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 249.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 267.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 204.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 203.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 255.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 222.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 255.7 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 300.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 203.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 255.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 240.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 343.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 239.7 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 59.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 281.2 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 239.7 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 267.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 218.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 51.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 218.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 179.8 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 218.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 179.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 204.6 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 348.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 218.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TbCoSi (mp-22206) | 0.1668 | 0.028 | 3 |
TbSiRu (mp-20645) | 0.1418 | 0.000 | 3 |
HoCoSi (mp-510688) | 0.1455 | 0.000 | 3 |
DyCoSi (mp-19767) | 0.1349 | 0.000 | 3 |
DySiRu (mp-19873) | 0.1611 | 0.000 | 3 |
Mg2Ga5 (mp-27668) | 0.6905 | 0.000 | 2 |
PbCl2 (mp-619071) | 0.6385 | 0.023 | 2 |
Cs4Pb9 (mp-574070) | 0.7125 | 0.000 | 2 |
MgSi2 (mp-1073663) | 0.6937 | 0.232 | 2 |
MgSi (mp-1073829) | 0.6786 | 0.166 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Ge_d Rh_pv |
Final Energy/Atom-5.3915 eV |
Corrected Energy-64.6986 eV
Uncorrected energy = -64.6986 eV
Corrected energy = -64.6986 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)