Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.303 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.311 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3Sn2 + Sn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 101.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 146.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 231.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 57.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 62.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 125.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 83.6 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 116.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 152.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 289.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 101.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 144.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 57.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 76.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 216.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 274.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 83.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 188.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 83.6 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 116.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 83.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 274.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 304.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 231.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 271.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 216.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 188.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 101.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 144.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 57.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 50.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 188.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 14.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 144.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 72.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 208.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 127.0 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 216.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 155.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 202.4 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 83.6 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 127.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 231.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 43.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 216.9 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 50.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 228.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 173.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 173.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 180.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
138 | 50 | 51 | 0 | 0 | 0 |
50 | 138 | 51 | 0 | 0 | 0 |
51 | 51 | 183 | 0 | 0 | 0 |
0 | 0 | 0 | 83 | 0 | 0 |
0 | 0 | 0 | 0 | 83 | 0 |
0 | 0 | 0 | 0 | 0 | 44 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.8 | -2.6 | -1.7 | 0 | 0 | 0 |
-2.6 | 8.8 | -1.7 | 0 | 0 | 0 |
-1.7 | -1.7 | 6.4 | 0 | 0 | 0 |
0 | 0 | 0 | 12.1 | 0 | 0 |
0 | 0 | 0 | 0 | 12.1 | 0 |
0 | 0 | 0 | 0 | 0 | 22.8 |
Shear Modulus GV62 GPa |
Bulk Modulus KV85 GPa |
Shear Modulus GR57 GPa |
Bulk Modulus KR83 GPa |
Shear Modulus GVRH60 GPa |
Bulk Modulus KVRH84 GPa |
Elastic Anisotropy0.45 |
Poisson's Ratio0.21 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2SbTe (mp-675700) | 0.5110 | 0.325 | 3 |
Cr2AsSe (mp-676270) | 0.6146 | 0.304 | 3 |
Ni2SbTe (mp-676310) | 0.2329 | 0.010 | 3 |
Co2SbTe (mp-675568) | 0.3909 | 0.043 | 3 |
CuNiSb2 (mp-11834) | 0.3701 | 0.002 | 3 |
BRh (mp-567164) | 0.0279 | 0.000 | 2 |
NiPb (mp-569446) | 0.0053 | 0.087 | 2 |
BiPt (mp-1066078) | 0.0416 | 0.000 | 2 |
FeTe (mp-10761) | 0.0423 | 0.332 | 2 |
FeSb (mp-2619) | 0.0032 | 0.107 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv Sn_d |
Final Energy/Atom-5.9275 eV |
Corrected Energy-23.7101 eV
-23.7101 eV = -23.7101 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)