Final Magnetic Moment2.565 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 77.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 273.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 77.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 349.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 272.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 273.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 311.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 311.0 |
BN (mp-984) | <1 1 1> | <1 0 1> | 236.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 68.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 194.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 116.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 311.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 311.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 194.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 329.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 205.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 274.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 273.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 194.4 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 219.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 311.0 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 77.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 349.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 329.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 116.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 274.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 274.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 272.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 194.4 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 55.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 68.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 194.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 116.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 194.4 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 272.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 77.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 205.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 274.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 311.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 116.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 233.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 272.1 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 273.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 236.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 194.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 272.1 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 311.0 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 274.9 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 194.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(Mn2Fe)4 (mp-982188) | 0.2120 | 0.019 | 3 |
Er(SiNi5)2 (mp-21548) | 0.5648 | 0.000 | 3 |
Ho(SiNi5)2 (mp-542390) | 0.5646 | 0.000 | 3 |
Pr(Al2Cu)4 (mp-862763) | 0.5637 | 0.000 | 3 |
Ca(Al2Cu)4 (mp-10877) | 0.5569 | 0.000 | 3 |
NdMn12 (mp-20642) | 0.1130 | 0.051 | 2 |
ErMn12 (mp-22482) | 0.1207 | 0.000 | 2 |
YMn12 (mp-22508) | 0.0172 | 0.000 | 2 |
HoMn12 (mp-14015) | 0.0167 | 0.000 | 2 |
ThMn12 (mp-31221) | 0.1106 | 0.044 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Mn_pv |
Final Energy/Atom-8.8155 eV |
Corrected Energy-114.6014 eV
-114.6014 eV = -114.6014 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)