Final Magnetic Moment0.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.212 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn4Al11 + MnAl + UAl2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 63.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 135.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 254.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 153.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 225.1 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 191.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 225.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 315.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 307.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 76.9 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 135.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 135.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 45.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 225.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 315.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 315.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 318.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 307.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 76.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 307.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 267.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 135.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 199.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 254.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 315.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 254.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 270.2 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 191.0 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 191.0 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 254.7 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 199.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 270.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 191.0 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 254.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 270.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 270.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 153.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 135.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 270.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 191.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 270.2 |
BN (mp-984) | <1 0 0> | <1 1 0> | 191.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 135.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 135.1 |
Al (mp-134) | <1 1 1> | <1 1 1> | 199.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 191.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 135.1 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 267.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 307.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 270.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er(Al2Fe)4 (mp-3633) | 0.1314 | 0.000 | 3 |
Sc(Al2Fe)4 (mp-3701) | 0.1252 | 0.000 | 3 |
Lu(Al2Fe)4 (mp-11037) | 0.1199 | 0.000 | 3 |
Y(Al2Fe)4 (mp-4656) | 0.1345 | 0.000 | 3 |
Ce(MnAl2)4 (mp-16487) | 0.1047 | 0.024 | 3 |
Be12V (mp-571438) | 0.4884 | 0.000 | 2 |
Be12Pt (mp-571622) | 0.3737 | 0.119 | 2 |
Be12Au (mp-12664) | 0.3883 | 0.114 | 2 |
Be12Pd (mp-12666) | 0.3747 | 0.079 | 2 |
Be12Cr (mp-1590) | 0.4926 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Mn_pv Al |
Final Energy/Atom-6.2045 eV |
Corrected Energy-80.6586 eV
-80.6586 eV = -80.6586 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)