material

TiCu

ID:

mp-2078

DOI:

10.17188/1195970


Tags: Copper titanium (1/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.136 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 103128 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaSe (mp-1943) <1 1 0> <1 1 0> 0.000 234.6
GaTe (mp-542812) <1 0 1> <1 0 0> 0.002 294.9
SrTiO3 (mp-4651) <1 1 1> <1 1 0> 0.003 208.5
PbSe (mp-2201) <1 0 0> <0 0 1> 0.003 38.9
Mg (mp-153) <1 1 0> <1 0 0> 0.004 202.7
Au (mp-81) <1 1 0> <1 0 0> 0.007 73.7
AlN (mp-661) <1 0 0> <1 0 1> 0.014 62.5
GaSb (mp-1156) <1 0 0> <0 0 1> 0.014 38.9
Ag (mp-124) <1 1 0> <1 0 0> 0.016 73.7
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.016 55.3
Au (mp-81) <1 0 0> <0 0 1> 0.016 87.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.016 87.4
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.017 126.3
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.022 78.2
AlN (mp-661) <0 0 1> <0 0 1> 0.023 68.0
InSb (mp-20012) <1 0 0> <0 0 1> 0.026 87.4
Cu (mp-30) <1 1 0> <1 0 1> 0.026 166.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.027 29.1
CdSe (mp-2691) <1 0 0> <0 0 1> 0.029 38.9
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.036 166.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.037 204.0
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.038 126.3
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.040 87.4
InSb (mp-20012) <1 1 0> <1 0 1> 0.041 62.5
C (mp-66) <1 1 1> <1 1 1> 0.041 111.3
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.043 194.3
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.045 139.1
Ga2O3 (mp-886) <0 1 0> <1 1 0> 0.047 286.7
CdTe (mp-406) <1 1 0> <1 0 1> 0.050 62.5
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.051 111.3
MgAl2O4 (mp-3536) <1 1 0> <1 0 1> 0.052 187.5
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.052 281.8
Au (mp-81) <1 1 1> <1 1 0> 0.064 182.4
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.064 87.4
Ag (mp-124) <1 0 0> <0 0 1> 0.065 87.4
GaN (mp-804) <1 1 0> <1 0 0> 0.069 202.7
CdS (mp-672) <0 0 1> <1 1 1> 0.070 139.1
Bi2Te3 (mp-34202) <1 0 1> <1 1 1> 0.072 139.1
SiC (mp-11714) <1 0 0> <1 0 1> 0.073 62.5
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.077 204.0
SiC (mp-11714) <1 0 1> <1 0 0> 0.086 129.0
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.100 92.2
SiC (mp-8062) <1 0 0> <0 0 1> 0.105 19.4
Ga2O3 (mp-886) <1 1 0> <1 1 1> 0.107 222.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.111 77.7
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.111 38.9
Ni (mp-23) <1 0 0> <0 0 1> 0.111 48.6
MoSe2 (mp-1634) <1 0 0> <1 0 1> 0.114 104.2
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.116 242.9
TePb (mp-19717) <1 0 0> <0 0 1> 0.121 87.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
178 103 107 0 0 0
103 178 107 0 0 0
107 107 186 0 0 0
0 0 0 85 0 0
0 0 0 0 85 0
0 0 0 0 0 89
Compliance Tensor Sij (10-12Pa-1)
9.8 -3.5 -3.6 0 0 0
-3.5 9.8 -3.6 0 0 0
-3.6 -3.6 9.6 0 0 0
0 0 0 11.8 0 0
0 0 0 0 11.8 0
0 0 0 0 0 11.3
Shear Modulus GV
67 GPa
Bulk Modulus KV
131 GPa
Shear Modulus GR
57 GPa
Bulk Modulus KR
130 GPa
Shear Modulus GVRH
62 GPa
Bulk Modulus KVRH
130 GPa
Elastic Anisotropy
0.87
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiFeP (mp-1008925) 0.5762 0.314 3
HfAu (mp-1007755) 0.6070 0.000 2
HfAg (mp-13156) 0.4170 0.000 2
AlCr2 (mp-1699) 0.6368 0.000 2
ZrAg (mp-11239) 0.1919 0.000 2
U2Mo (mp-30789) 0.6355 0.069 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Cu_pv
Final Energy/Atom
-6.1332 eV
Corrected Energy
-24.5326 eV
-24.5326 eV = -24.5326 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 600100
  • 629389
  • 103128
  • 629381
Submitted by
User remarks:
  • Copper titanium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)