material

Ga2FeS4

ID:

mp-20793

DOI:

10.17188/1195983


Tags: Iron digallium tetrasulfide - alpha Iron(II) gallium(III) sulfide (1/2/4)

Material Details

Final Magnetic Moment
4.009 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.808 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.097 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
FeS + Ga2S3
Band Gap
0.440 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 1> <0 0 1> 0.003 220.3
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.007 328.1
GaN (mp-804) <1 0 0> <1 0 0> 0.008 136.2
BN (mp-984) <0 0 1> <0 0 1> 0.009 104.3
GaTe (mp-542812) <0 0 1> <1 0 0> 0.009 227.0
GaSe (mp-1943) <0 0 1> <0 0 1> 0.010 150.7
Ni (mp-23) <1 1 0> <1 0 0> 0.010 227.0
Te2W (mp-22693) <0 0 1> <1 1 0> 0.011 157.3
Ge (mp-32) <1 0 0> <1 0 1> 0.011 234.3
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.012 227.0
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.012 140.6
BN (mp-984) <1 0 1> <0 0 1> 0.012 220.3
Mg (mp-153) <1 0 1> <0 0 1> 0.015 150.7
InP (mp-20351) <1 1 1> <0 0 1> 0.015 185.5
Mg (mp-153) <1 0 0> <1 0 0> 0.020 136.2
PbS (mp-21276) <1 0 0> <1 0 1> 0.023 328.1
GaAs (mp-2534) <1 0 0> <1 0 1> 0.027 234.3
GaP (mp-2490) <1 0 0> <0 0 1> 0.029 243.5
WS2 (mp-224) <1 1 0> <0 0 1> 0.031 313.0
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.031 314.6
CdS (mp-672) <0 0 1> <0 0 1> 0.031 46.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.036 185.5
Mg (mp-153) <0 0 1> <0 0 1> 0.037 34.8
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.039 185.5
WS2 (mp-224) <1 1 1> <0 0 1> 0.039 313.0
ZnSe (mp-1190) <1 0 0> <1 0 1> 0.041 234.3
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.046 313.0
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.052 173.9
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.053 78.6
NaCl (mp-22862) <1 0 0> <1 1 0> 0.053 157.3
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.057 173.9
Y3Fe5O12 (mp-19648) <1 0 0> <1 1 0> 0.057 157.3
CdS (mp-672) <1 0 0> <1 0 1> 0.059 234.3
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.064 313.0
LaF3 (mp-905) <1 0 0> <1 0 0> 0.065 272.4
Mg (mp-153) <1 1 1> <0 0 1> 0.069 243.5
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.070 46.4
YVO4 (mp-19133) <1 1 0> <1 1 0> 0.072 314.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.073 150.7
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.074 104.3
LaF3 (mp-905) <1 1 0> <1 0 0> 0.075 90.8
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.078 34.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.078 34.8
KCl (mp-23193) <1 1 0> <1 0 1> 0.080 234.3
TiO2 (mp-390) <1 0 1> <1 0 1> 0.082 281.2
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.082 272.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.085 81.2
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.089 46.4
C (mp-48) <1 0 0> <1 0 0> 0.089 227.0
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.095 243.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
99 28 3 1 0 0
28 99 3 -1 0 0
3 3 9 0 0 0
1 -1 0 2 0 0
0 0 0 0 2 1
0 0 0 0 1 35
Compliance Tensor Sij (10-12Pa-1)
11.2 -3.2 -2.5 -8.9 0 0
-3.2 11.2 -2.5 8.9 0 0
-2.5 -2.5 110 0 0 0
-8.9 8.9 0 457.8 0 0
0 0 0 0 457.8 -17.8
0 0 0 0 -17.8 28.9
Shear Modulus GV
20 GPa
Bulk Modulus KV
30 GPa
Shear Modulus GR
4 GPa
Bulk Modulus KR
9 GPa
Shear Modulus GVRH
12 GPa
Bulk Modulus KVRH
19 GPa
Elastic Anisotropy
19.61
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr(GaS2)2 (mp-985304) 0.2367 0.070 3
Zn(GaS2)2 (mp-1094008) 0.1517 0.095 3
Mg(InSe2)2 (mp-1006591) 0.2463 0.000 3
Al2ZnS4 (mp-1096816) 0.1881 0.116 3
Mg(AlSe2)2 (mp-9479) 0.2054 0.021 3
Li3Mn5Cr3O16 (mp-775496) 0.5168 0.005 4
CdInGaS4 (mp-630773) 0.3309 0.084 4
Li2Fe3O3F5 (mp-849525) 0.5781 0.109 4
LiMn3CrO8 (mp-773299) 0.5770 0.011 4
Li7Mn10Cr6O32 (mp-769505) 0.5590 0.004 4
Fe21O32 (mp-698578) 0.6630 0.195 2
Co2S3 (mp-684732) 0.5638 0.026 2
Co23O32 (mp-705564) 0.6079 0.000 2
Co29O40 (mp-705563) 0.6452 0.095 2
Co5O8 (mp-761471) 0.5723 0.024 2
Li4Nb3Fe3(SbO8)2 (mp-868012) 0.7214 0.067 5
Li4Cr3Cu2Sb3O16 (mp-775356) 0.7117 0.106 5
Li4Mn3Nb3(SbO8)2 (mp-773620) 0.7432 0.086 5
Li4Fe3Cu2Sb3O16 (mp-765704) 0.7064 0.107 5
Li4Nb3Fe3(TeO8)2 (mp-779209) 0.7417 0.092 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ga_d Fe_pv S
Final Energy/Atom
-4.9599 eV
Corrected Energy
-36.7312 eV
Uncorrected energy = -34.7192 eV Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV Corrected energy = -36.7312 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 100706
  • 602041
Submitted by
User remarks:
  • Iron digallium tetrasulfide - alpha

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)