material

MnCo2Sn

ID:

mp-20840

DOI:

10.17188/1196041


Tags: Cobalt manganese tin (2/1/1)

Material Details

Final Magnetic Moment
5.009 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.125 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 102531 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.006 215.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.013 143.6
PbS (mp-21276) <1 0 0> <1 0 0> 0.013 35.9
PbS (mp-21276) <1 1 0> <1 1 0> 0.014 50.8
PbS (mp-21276) <1 1 1> <1 1 1> 0.015 62.2
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.021 152.3
MgO (mp-1265) <1 1 1> <1 0 0> 0.022 251.2
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.040 323.0
WS2 (mp-224) <0 0 1> <1 1 1> 0.045 62.2
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.045 62.2
TiO2 (mp-390) <0 0 1> <1 0 0> 0.064 71.8
GaN (mp-804) <0 0 1> <1 1 1> 0.066 62.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.072 35.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.076 304.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.077 50.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.090 251.2
C (mp-48) <0 0 1> <1 0 0> 0.090 251.2
InP (mp-20351) <1 0 0> <1 0 0> 0.101 35.9
InP (mp-20351) <1 1 0> <1 1 0> 0.109 50.8
ZnO (mp-2133) <1 0 1> <1 0 0> 0.111 215.3
InP (mp-20351) <1 1 1> <1 1 1> 0.112 62.2
Mg (mp-153) <0 0 1> <1 1 1> 0.115 62.2
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.118 179.5
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.126 251.2
SiC (mp-11714) <0 0 1> <1 0 0> 0.127 287.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.127 287.1
KCl (mp-23193) <1 0 0> <1 0 0> 0.130 323.0
SiC (mp-7631) <0 0 1> <1 0 0> 0.137 287.1
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.162 71.8
CdS (mp-672) <0 0 1> <1 1 1> 0.168 62.2
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.175 101.5
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.181 251.2
NaCl (mp-22862) <1 0 0> <1 0 0> 0.185 287.1
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.191 152.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.195 186.5
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.209 323.0
AlN (mp-661) <1 0 1> <1 1 0> 0.234 253.8
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.243 186.5
ZnO (mp-2133) <1 0 0> <1 1 1> 0.243 310.8
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.246 179.5
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.252 358.9
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.253 358.9
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.268 143.6
InSb (mp-20012) <1 0 0> <1 0 0> 0.290 179.5
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.290 203.0
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.296 248.7
Ag (mp-124) <1 1 1> <1 0 0> 0.305 179.5
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.309 358.9
AlN (mp-661) <1 1 1> <1 1 0> 0.324 203.0
ZnO (mp-2133) <1 1 1> <1 0 0> 0.327 287.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
232 136 136 0 0 0
136 232 136 0 0 0
136 136 232 0 0 0
0 0 0 109 0 0
0 0 0 0 109 0
0 0 0 0 0 109
Compliance Tensor Sij (10-12Pa-1)
7.6 -2.8 -2.8 0 0 0
-2.8 7.6 -2.8 0 0 0
-2.8 -2.8 7.6 0 0 0
0 0 0 9.2 0 0
0 0 0 0 9.2 0
0 0 0 0 0 9.2
Shear Modulus GV
84 GPa
Bulk Modulus KV
168 GPa
Shear Modulus GR
72 GPa
Bulk Modulus KR
168 GPa
Shear Modulus GVRH
78 GPa
Bulk Modulus KVRH
168 GPa
Elastic Anisotropy
0.85
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiAlFe2 (mp-31187) 0.0000 0.000 3
TiGaNi2 (mp-30657) 0.0000 0.000 3
CrGaFe2 (mp-30570) 0.0000 0.087 3
MnAlPt2 (mp-10893) 0.0000 0.448 3
ScSnPt2 (mp-30844) 0.0000 0.052 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
SmMg3 (mp-30779) 0.0000 0.065 2
Ni3Sb (mp-10260) 0.0000 0.044 2
Li3Au (mp-11247) 0.0000 0.000 2
Li3Pd (mp-11489) 0.0000 0.001 2
Cu3Sb (mp-2002) 0.0000 0.181 2
Er (mp-10753) 0.0000 0.143 1
Nd (mp-4) 0.0000 0.140 1
Tm (mp-10661) 0.0000 0.140 1
Ho (mp-7236) 0.0000 0.145 1
Pb (mp-22692) 0.0000 0.048 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Co Sn_d
Final Energy/Atom
-6.9678 eV
Corrected Energy
-27.8713 eV
Uncorrected energy = -27.8713 eV Corrected energy = -27.8713 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 624165
  • 102531
  • 624172
  • 624169
  • 624177
  • 624166
  • 624173
  • 102532
  • 624171
Submitted by
User remarks:
  • Cobalt manganese tin (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)