Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.032 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPr2Co17 + Pr5Co2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 305.5 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 229.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 270.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 270.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 229.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 280.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 270.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 229.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 280.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 305.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 305.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 152.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 216.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 229.1 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 280.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 270.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 229.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 280.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 270.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 216.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 229.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 54.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 229.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 216.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 324.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 216.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 152.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 216.0 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 280.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 270.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 270.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 270.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 93.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 270.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 305.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 216.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 229.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 270.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 270.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 270.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 324.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 216.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 93.5 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 76.4 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 93.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 108.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 108.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 152.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 216.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 305.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
140 | 108 | 108 | 6 | 5 | -5 |
108 | 140 | 108 | 5 | 6 | -5 |
108 | 108 | 140 | 5 | 5 | -6 |
6 | 5 | 5 | 22 | 0 | 0 |
5 | 6 | 5 | 0 | 22 | 0 |
-5 | -5 | -6 | 0 | 0 | 22 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
22.2 | -9.7 | -9.7 | -1.2 | -0.5 | 0.5 |
-9.7 | 22.2 | -9.7 | -0.5 | -1.2 | 0.5 |
-9.7 | -9.7 | 22.2 | -0.5 | -0.5 | 1.2 |
-1.2 | -0.5 | -0.5 | 47.1 | 0.6 | -0.6 |
-0.5 | -1.2 | -0.5 | 0.6 | 47.1 | -0.6 |
0.5 | 0.5 | 1.2 | -0.6 | -0.6 | 47.1 |
Shear Modulus GV19 GPa |
Bulk Modulus KV119 GPa |
Shear Modulus GR19 GPa |
Bulk Modulus KR114 GPa |
Shear Modulus GVRH19 GPa |
Bulk Modulus KVRH117 GPa |
Elastic Anisotropy0.19 |
Poisson's Ratio0.42 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
EuAl2 (mp-917786) | 0.0000 | 0.000 | 2 |
SmCo2 (mp-1071998) | 0.0000 | 0.022 | 2 |
HoFe2 (mp-1077795) | 0.0000 | 0.157 | 2 |
NbNi2 (mp-1077429) | 0.0000 | 0.083 | 2 |
SmFe2 (mp-913717) | 0.0000 | 0.022 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Co |
Final Energy/Atom-6.3007 eV |
Corrected Energy-37.8042 eV
-37.8042 eV = -37.8042 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)