Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.534 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.555 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGeO2 |
Band Gap0.997 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3121 [152] |
HallP 31 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 340.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 139.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 294.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 134.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 107.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 241.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 26.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 232.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 232.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 214.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 149.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 294.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 136.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 276.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 294.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 255.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 26.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 34.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 46.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 51.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 276.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 92.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 53.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 214.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 324.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 294.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 273.7 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 102.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 171.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 214.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 324.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 149.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 294.7 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 102.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 85.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 149.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 149.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 276.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 276.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 63.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 63.9 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 276.7 |
Al (mp-134) | <1 0 0> | <1 0 1> | 273.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 160.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 107.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 191.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 63.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 191.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbSnF3 (mp-998620) | 0.5682 | 0.013 | 3 |
GdAsO3 (mp-753953) | 0.4626 | 0.055 | 3 |
NbBiO4 (mp-863076) | 0.4666 | 0.066 | 3 |
BiSbO3 (mp-755382) | 0.5813 | 0.086 | 3 |
NbBiO4 (mp-23413) | 0.5725 | 0.005 | 3 |
InAg(WO4)2 (mp-614383) | 0.6744 | 0.018 | 4 |
Na2MoSeO6 (mp-567030) | 0.6488 | 0.000 | 4 |
InCu(MoO4)2 (mp-618075) | 0.6412 | 0.037 | 4 |
NaIn(WO4)2 (mp-25649) | 0.6718 | 0.000 | 4 |
YAg(WO4)2 (mvc-653) | 0.6149 | 0.009 | 4 |
Te3Cl2 (mp-27628) | 0.6831 | 0.013 | 2 |
IrC2 (mp-1077889) | 0.7188 | 1.292 | 2 |
CoO2 (mp-1062643) | 0.7044 | 0.521 | 2 |
WN2 (mp-776321) | 0.7004 | 0.143 | 2 |
SbF3 (mp-1880) | 0.7342 | 0.000 | 2 |
Explore more synthesis descriptions for materials of composition GeO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d O |
Final Energy/Atom-5.0614 eV |
Corrected Energy-48.3502 eV
-48.3502 eV = -45.5528 eV (uncorrected energy) - 2.7973 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)