Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.420 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 122.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 122.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 173.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 281.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 122.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 150.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 173.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 195.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 337.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 151.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 337.0 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 122.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 150.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 245.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 173.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 61.3 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 216.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 91.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 281.6 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 262.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 245.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 337.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 173.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 91.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 262.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 112.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 337.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 108.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 238.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 238.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 91.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 245.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 108.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 43.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 187.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 43.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 61.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 337.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 195.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 262.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 91.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 216.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 86.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 275.7 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 262.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 150.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 91.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 337.0 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 214.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 86.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
91 | 31 | 31 | 0 | 0 | 0 |
31 | 91 | 31 | 0 | 0 | 0 |
31 | 31 | 91 | 0 | 0 | 0 |
0 | 0 | 0 | 25 | 0 | 0 |
0 | 0 | 0 | 0 | 25 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.3 | -3.4 | -3.4 | 0 | 0 | 0 |
-3.4 | 13.3 | -3.4 | 0 | 0 | 0 |
-3.4 | -3.4 | 13.3 | 0 | 0 | 0 |
0 | 0 | 0 | 40 | 0 | 0 |
0 | 0 | 0 | 0 | 40 | 0 |
0 | 0 | 0 | 0 | 0 | 40 |
Shear Modulus GV27 GPa |
Bulk Modulus KV51 GPa |
Shear Modulus GR27 GPa |
Bulk Modulus KR51 GPa |
Shear Modulus GVRH27 GPa |
Bulk Modulus KVRH51 GPa |
Elastic Anisotropy0.04 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Pt3Pb (mp-20828) | 0.0000 | 0.034 | 2 |
MnCo3 (mp-999563) | 0.0000 | 0.048 | 2 |
PuRh3 (mp-1678) | 0.0000 | 0.000 | 2 |
PuSn3 (mp-2279) | 0.0000 | 0.448 | 2 |
GdSn3 (mp-19919) | 0.0000 | 0.000 | 2 |
Sr (mp-76) | 0.0000 | 0.006 | 1 |
Mg (mp-1056702) | 0.0000 | 0.014 | 1 |
N2 (mp-1056857) | 0.0000 | 0.000 | 1 |
Ni (mp-1056486) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.001 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 In_d |
Final Energy/Atom-3.6426 eV |
Corrected Energy-14.5703 eV
-14.5703 eV = -14.5703 eV (uncorrected energy)
|