material

V2InC

ID:

mp-20983

DOI:

10.17188/1196217


Tags: High pressure experimental phase Vanadium indium carbide (2/1/1)

Material Details

Final Magnetic Moment
0.011 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.344 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.04 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
V2C + In
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 1 1> <0 0 1> 0.000 245.7
Al (mp-134) <1 1 1> <0 0 1> 0.002 198.1
InAs (mp-20305) <1 1 1> <0 0 1> 0.004 198.1
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.009 198.1
BN (mp-984) <0 0 1> <0 0 1> 0.010 71.3
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.012 221.9
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.022 126.8
AlN (mp-661) <1 1 1> <1 1 0> 0.025 142.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.025 198.1
GaSe (mp-1943) <0 0 1> <0 0 1> 0.028 150.6
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.028 198.1
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.029 221.9
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.031 23.8
KCl (mp-23193) <1 1 1> <0 0 1> 0.036 71.3
LiTaO3 (mp-3666) <1 0 1> <0 0 1> 0.042 229.8
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.042 209.6
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.044 142.6
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.046 288.2
GaN (mp-804) <1 0 0> <0 0 1> 0.050 150.6
MgO (mp-1265) <1 0 0> <0 0 1> 0.050 126.8
Ni (mp-23) <1 1 1> <0 0 1> 0.065 150.6
MgO (mp-1265) <1 1 1> <0 0 1> 0.080 31.7
Mg (mp-153) <1 0 0> <0 0 1> 0.086 150.6
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.088 190.2
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.102 221.9
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.103 71.3
NaCl (mp-22862) <1 1 1> <0 0 1> 0.106 55.5
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.109 245.7
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.112 23.8
GaTe (mp-542812) <0 1 0> <0 0 1> 0.113 190.2
CdSe (mp-2691) <1 1 1> <0 0 1> 0.122 198.1
AlN (mp-661) <0 0 1> <0 0 1> 0.126 103.0
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.148 142.6
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.149 31.7
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.157 324.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.166 198.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.169 150.6
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.170 221.9
C (mp-48) <1 1 1> <0 0 1> 0.171 166.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.187 103.0
Te2W (mp-22693) <1 0 0> <0 0 1> 0.187 293.2
DyScO3 (mp-31120) <0 1 1> <0 0 1> 0.191 324.9
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.212 221.9
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.217 47.5
Mg (mp-153) <1 1 0> <1 1 0> 0.218 142.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.233 126.8
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.235 126.8
AlN (mp-661) <1 1 0> <0 0 1> 0.237 324.9
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.241 166.4
WS2 (mp-224) <1 1 0> <0 0 1> 0.259 309.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
300 78 90 0 0 0
78 300 90 0 0 0
90 90 270 0 0 0
0 0 0 101 0 0
0 0 0 0 101 0
0 0 0 0 0 111
Compliance Tensor Sij (10-12Pa-1)
3.8 -0.7 -1 0 0 0
-0.7 3.8 -1 0 0 0
-1 -1 4.4 0 0 0
0 0 0 9.9 0 0
0 0 0 0 9.9 0
0 0 0 0 0 9
Shear Modulus GV
103 GPa
Bulk Modulus KV
154 GPa
Shear Modulus GR
103 GPa
Bulk Modulus KR
154 GPa
Shear Modulus GVRH
103 GPa
Bulk Modulus KVRH
154 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ti2InC (mp-20315) 0.0339 0.000 3
Sc2TlC (mp-13071) 0.0876 0.010 3
Ti2TlC (mp-1092281) 0.0280 0.000 3
Sc2InC (mp-20175) 0.1198 0.013 3
Ti2InN (mp-1025517) 0.0964 0.000 3
Co3H (mp-1025425) 0.3435 0.182 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv In_d C
Final Energy/Atom
-7.8795 eV
Corrected Energy
-63.0357 eV
-63.0357 eV = -63.0357 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 163514
  • 163505
  • 163515
Submitted by
User remarks:
  • High pressure experimental phase
  • Vanadium indium carbide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)