Final Magnetic Moment3.296 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.197 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeAs + Ce |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 112.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 79.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 112.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 79.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 112.1 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 158.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 317.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 79.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 112.1 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 237.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 137.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 158.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 158.5 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 224.2 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 317.1 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 237.8 |
BN (mp-984) | <0 0 1> | <1 1 0> | 224.2 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 79.3 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 112.1 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 158.5 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 317.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 237.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 137.3 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 112.1 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 224.2 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 79.3 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 112.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 237.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 317.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 237.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 317.1 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 317.1 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 137.3 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 317.1 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 317.1 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 317.1 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 158.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 79.3 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 112.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 79.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 317.1 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 224.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 158.5 |
Au (mp-81) | <1 1 0> | <1 1 0> | 224.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 79.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm(GdS2)2 (mp-676424) | 0.1225 | 0.027 | 3 |
Nd(SmSb)3 (mp-675554) | 0.0437 | 0.007 | 3 |
Tb2SmS4 (mp-38931) | 0.1085 | 0.062 | 3 |
Sm(DyS2)2 (mp-34987) | 0.1163 | 0.070 | 3 |
Ca(Sm2Se3)4 (mp-34196) | 0.1219 | 0.033 | 3 |
Nd4Sb3 (mp-530) | 0.0108 | 0.000 | 2 |
Pr4Bi3 (mp-23314) | 0.0187 | 0.011 | 2 |
Sm4Sn3 (mp-571474) | 0.0037 | 0.000 | 2 |
Pr4Sb3 (mp-1484) | 0.0093 | 0.000 | 2 |
La4Sb3 (mp-1223) | 0.0165 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce As |
Final Energy/Atom-6.5841 eV |
Corrected Energy-92.1768 eV
-92.1768 eV = -92.1768 eV (uncorrected energy)
|