material

Si3Rh5

ID:

mp-21012

DOI:

10.17188/1196256


Tags: Rhodium silicide (5/3)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.748 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.027 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.14 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SiRh2 + Si2Rh3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pbam [55]
Hall
-P 2 2ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 43338 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.005 206.0
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.018 147.7
LiAlO2 (mp-3427) <0 0 1> <0 1 1> 0.021 136.5
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.025 274.3
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.032 287.4
SiC (mp-11714) <1 1 1> <1 1 0> 0.033 274.7
C (mp-66) <1 1 1> <1 1 1> 0.036 287.4
Au (mp-81) <1 1 1> <0 1 0> 0.047 120.9
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.047 211.0
C (mp-48) <1 1 0> <1 0 0> 0.048 166.8
Au (mp-81) <1 1 0> <1 0 0> 0.049 222.4
BN (mp-984) <1 1 1> <0 0 1> 0.054 168.8
WS2 (mp-224) <1 0 1> <0 0 1> 0.058 232.1
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.063 166.8
InAs (mp-20305) <1 0 0> <0 1 1> 0.068 227.5
TiO2 (mp-390) <1 1 0> <0 0 1> 0.072 105.5
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.075 206.0
GdScO3 (mp-5690) <1 0 1> <0 1 1> 0.085 227.5
ZnTe (mp-2176) <1 0 0> <0 1 1> 0.085 227.5
Ag (mp-124) <1 1 1> <0 1 0> 0.087 120.9
GaN (mp-804) <0 0 1> <1 0 1> 0.089 178.4
NdGaO3 (mp-3196) <1 1 0> <0 1 1> 0.098 182.0
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.104 161.2
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.111 168.8
LaF3 (mp-905) <1 0 1> <1 0 0> 0.117 278.0
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.122 105.5
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.128 105.5
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.130 59.5
GaN (mp-804) <1 0 1> <0 0 1> 0.130 189.9
LiGaO2 (mp-5854) <1 0 1> <1 0 1> 0.131 178.4
Si (mp-149) <1 0 0> <1 0 1> 0.134 59.5
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.134 55.6
SiC (mp-8062) <1 0 0> <0 1 1> 0.141 227.5
KTaO3 (mp-3614) <1 0 0> <0 1 1> 0.142 273.0
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.146 274.3
Si (mp-149) <1 1 0> <0 0 1> 0.153 42.2
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.153 42.2
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.154 232.1
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.160 137.4
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.161 278.0
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.164 42.2
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.166 287.4
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.168 278.0
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.177 137.4
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.182 55.6
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.183 201.6
Ni (mp-23) <1 1 0> <0 0 1> 0.185 189.9
Mg (mp-153) <1 0 1> <0 0 1> 0.187 189.9
Cu (mp-30) <1 0 0> <1 0 1> 0.204 119.0
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.207 119.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
250 142 182 0 0 0
142 236 181 0 0 0
182 181 357 0 0 0
0 0 0 94 0 0
0 0 0 0 114 0
0 0 0 0 0 77
Compliance Tensor Sij (10-12Pa-1)
7.2 -2.4 -2.4 0 0 0
-2.4 7.8 -2.7 0 0 0
-2.4 -2.7 5.4 0 0 0
0 0 0 10.6 0 0
0 0 0 0 8.8 0
0 0 0 0 0 12.9
Shear Modulus GV
80 GPa
Bulk Modulus KV
206 GPa
Shear Modulus GR
72 GPa
Bulk Modulus KR
191 GPa
Shear Modulus GVRH
76 GPa
Bulk Modulus KVRH
199 GPa
Elastic Anisotropy
0.61
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na2PrO3 (mp-685712) 0.7346 0.197 3
Ga2AsRh5 (mp-18561) 0.4191 0.000 3
Ge3Rh5 (mp-624221) 0.1776 0.012 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Rh_pv
Final Energy/Atom
-7.3854 eV
Corrected Energy
-118.1659 eV
Uncorrected energy = -118.1659 eV Corrected energy = -118.1659 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43338
  • 43679
  • 650299
Submitted by
User remarks:
  • Rhodium silicide (5/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)