material

HfC

ID:

mp-21075

DOI:

10.17188/1196352


Tags: Hafnium carbide (1/1) Hafnium carbide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.940 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 22262 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <1 1 1> 0.000 37.5
Ag (mp-124) <1 0 0> <1 0 0> 0.000 86.5
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.000 21.6
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.000 262.3
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.002 112.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.002 91.8
ZnO (mp-2133) <1 0 1> <1 0 0> 0.002 238.0
NaCl (mp-22862) <1 1 0> <1 1 0> 0.004 91.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.008 244.8
SiC (mp-7631) <1 1 0> <1 1 0> 0.008 244.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.008 173.1
TePb (mp-19717) <1 1 0> <1 1 0> 0.015 61.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.015 43.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.022 194.7
Ni (mp-23) <1 1 1> <1 1 1> 0.024 149.9
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.026 336.6
Al (mp-134) <1 1 1> <1 1 1> 0.033 112.4
Al (mp-134) <1 1 0> <1 1 0> 0.033 91.8
Au (mp-81) <1 0 0> <1 0 0> 0.033 86.5
SiC (mp-7631) <1 1 1> <1 1 0> 0.040 244.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.055 194.7
CdSe (mp-2691) <1 0 0> <1 0 0> 0.092 194.7
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.094 262.3
InAs (mp-20305) <1 1 1> <1 1 1> 0.098 262.3
WSe2 (mp-1821) <1 1 1> <1 1 1> 0.110 262.3
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.123 262.3
GaSe (mp-1943) <0 0 1> <1 1 1> 0.126 37.5
Cu (mp-30) <1 1 0> <1 1 0> 0.135 336.6
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.138 122.4
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.150 61.2
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.156 108.2
DyScO3 (mp-31120) <0 0 1> <1 1 1> 0.157 187.4
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.158 43.3
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.170 183.6
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.206 91.8
AlN (mp-661) <1 0 0> <1 0 0> 0.220 281.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.223 194.7
AlN (mp-661) <1 1 0> <1 1 0> 0.224 244.8
NaCl (mp-22862) <1 0 0> <1 1 1> 0.237 262.3
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.241 129.8
TbScO3 (mp-31119) <0 0 1> <1 1 1> 0.245 187.4
TiO2 (mp-390) <1 0 0> <1 1 0> 0.260 336.6
Mg (mp-153) <0 0 1> <1 1 1> 0.264 112.4
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.266 151.4
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.267 91.8
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.268 151.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.282 61.2
CdTe (mp-406) <1 0 0> <1 0 0> 0.287 43.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.300 91.8
BN (mp-984) <0 0 1> <1 1 0> 0.309 153.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
496 106 106 0 0 0
106 496 106 0 0 0
106 106 496 0 0 0
0 0 0 171 0 0
0 0 0 0 171 0
0 0 0 0 0 171
Compliance Tensor Sij (10-12Pa-1)
2.2 -0.4 -0.4 0 0 0
-0.4 2.2 -0.4 0 0 0
-0.4 -0.4 2.2 0 0 0
0 0 0 5.9 0 0
0 0 0 0 5.9 0
0 0 0 0 0 5.9
Shear Modulus GV
180 GPa
Bulk Modulus KV
236 GPa
Shear Modulus GR
179 GPa
Bulk Modulus KR
236 GPa
Shear Modulus GVRH
180 GPa
Bulk Modulus KVRH
236 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.114 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
GdN (mp-940) 0.0000 0.000 2
SrO (mp-2472) 0.0000 0.000 2
YbS (mp-1820) 0.0000 0.000 2
InTe (mp-2597) 0.0000 0.000 2
YbP (mp-2390) 0.0000 0.000 2
As (mp-10) 0.0000 0.112 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv C
Final Energy/Atom
-10.5318 eV
Corrected Energy
-21.0636 eV
Uncorrected energy = -21.0636 eV Corrected energy = -21.0636 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 618012
  • 618010
  • 618002
  • 658336
  • 618020
  • 618017
  • 180600
  • 618008
  • 185978
  • 618018
  • 181793
  • 618016
  • 108134
  • 618005
  • 22262
  • 618000
  • 618013
  • 617997
  • 618011
  • 658398
  • 618001
  • 617998
  • 618015
  • 618004
  • 159873
  • 192046
  • 618009
  • 618003
Submitted by
User remarks:
  • Hafnium carbide (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)