Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.543 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 193.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 265.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 126.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 204.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 190.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 319.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 217.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 169.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 48.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 191.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 144.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 217.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 144.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 72.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 319.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 319.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 289.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 313.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 313.8 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 190.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 217.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 190.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 273.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 253.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 362.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 86.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 362.1 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 259.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 255.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 190.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 175.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 217.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 191.5 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 191.5 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 217.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 175.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 193.1 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 255.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 175.7 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 217.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 265.5 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 191.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 255.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 190.1 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 273.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 126.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 126.7 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 126.7 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 126.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.5214 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.5711 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.5864 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.4823 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.6912 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.5061 | 0.106 | 4 |
CaSn (mp-2450) | 0.0548 | 0.000 | 2 |
LaSn (mp-1018047) | 0.1682 | 0.000 | 2 |
EuSn (mp-567833) | 0.1152 | 0.000 | 2 |
TbGe (mp-1405) | 0.2203 | 0.000 | 2 |
HoGe (mp-16342) | 0.2272 | 0.017 | 2 |
Si (mp-1001113) | 0.6736 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Pb_d |
Final Energy/Atom-3.2445 eV |
Corrected Energy-12.9778 eV
-12.9778 eV = -12.9778 eV (uncorrected energy)
|