Final Magnetic Moment1.707 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.462 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 285.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 305.0 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 305.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 217.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 301.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 126.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 285.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 79.3 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 261.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 190.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 229.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 57.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 237.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 79.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 174.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 284.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 172.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 57.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 79.3 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 174.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 284.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 238.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 284.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 126.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 63.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 79.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 217.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 31.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 285.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 142.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 222.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 284.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 284.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 15.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 114.8 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 57.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.8 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 348.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 206.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 237.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 237.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 324.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 206.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 202.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
206 | 75 | 102 | 0 | 0 | 0 |
75 | 206 | 102 | 0 | 0 | 0 |
102 | 102 | 166 | 0 | 0 | 0 |
0 | 0 | 0 | 69 | 0 | 0 |
0 | 0 | 0 | 0 | 69 | 0 |
0 | 0 | 0 | 0 | 0 | 57 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7 | -0.6 | -3.9 | 0 | 0 | 0 |
-0.6 | 7 | -3.9 | 0 | 0 | 0 |
-3.9 | -3.9 | 10.9 | 0 | 0 | 0 |
0 | 0 | 0 | 14.4 | 0 | 0 |
0 | 0 | 0 | 0 | 14.4 | 0 |
0 | 0 | 0 | 0 | 0 | 17.7 |
Shear Modulus GV59 GPa |
Bulk Modulus KV126 GPa |
Shear Modulus GR55 GPa |
Bulk Modulus KR126 GPa |
Shear Modulus GVRH57 GPa |
Bulk Modulus KVRH126 GPa |
Elastic Anisotropy0.38 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tb(CoGe)2 (mp-3709) | 0.0041 | 0.000 | 3 |
Dy(FeGe)2 (mp-21426) | 0.0078 | 0.000 | 3 |
Ho(CoGe)2 (mp-4415) | 0.0180 | 0.000 | 3 |
Dy(CoGe)2 (mp-19771) | 0.0058 | 0.000 | 3 |
Y(CoGe)2 (mp-4908) | 0.0053 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.5082 | 0.000 | 4 |
SrIn4 (mp-22466) | 0.2715 | 0.010 | 2 |
EuAl4 (mp-582799) | 0.2710 | 0.000 | 2 |
SrAl4 (mp-2775) | 0.1920 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.2036 | 0.000 | 2 |
RbIn4 (mp-21477) | 0.2487 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Fe_pv Ge_d |
Final Energy/Atom-6.9903 eV |
Corrected Energy-34.9513 eV
Uncorrected energy = -34.9513 eV
Corrected energy = -34.9513 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)