Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.902 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P213 [198]
Hall
P 2ac 2ab 3
Point Group
23
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-8062) <1 1 1> <1 1 1> 0.000 232.7
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.001 126.7
Si (mp-149) <1 1 0> <1 1 0> 0.002 126.7
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.008 223.9
BN (mp-984) <0 0 1> <1 1 1> 0.011 310.3
PbS (mp-21276) <1 0 0> <1 0 0> 0.020 179.1
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.022 190.0
Cu (mp-30) <1 0 0> <1 0 0> 0.028 223.9
LiF (mp-1138) <1 1 0> <1 1 0> 0.030 190.0
Ni (mp-23) <1 1 0> <1 1 0> 0.034 190.0
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.038 232.7
InP (mp-20351) <1 0 0> <1 0 0> 0.052 179.1
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.062 310.3
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.063 77.6
Ni (mp-23) <1 0 0> <1 0 0> 0.065 223.9
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.065 316.7
WS2 (mp-224) <0 0 1> <1 1 0> 0.065 316.7
WS2 (mp-224) <1 1 1> <1 1 0> 0.065 316.7
Mg (mp-153) <0 0 1> <1 1 0> 0.067 316.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.073 89.6
Ge (mp-32) <1 1 0> <1 1 0> 0.074 190.0
Ge (mp-32) <1 1 1> <1 1 1> 0.076 232.7
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.086 126.7
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.095 253.3
GaTe (mp-542812) <1 0 0> <1 1 0> 0.105 316.7
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.109 316.7
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.111 190.0
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.112 190.0
ZnO (mp-2133) <1 0 0> <1 0 0> 0.126 313.5
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.129 223.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.136 223.9
Mg (mp-153) <1 0 0> <1 1 0> 0.140 253.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.142 126.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.143 190.0
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.143 44.8
GaAs (mp-2534) <1 1 1> <1 1 1> 0.145 232.7
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.147 313.5
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.148 310.3
ZnO (mp-2133) <0 0 1> <1 0 0> 0.149 223.9
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.160 253.3
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.166 179.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.172 44.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.179 223.9
InSb (mp-20012) <1 1 0> <1 1 0> 0.181 63.3
InSb (mp-20012) <1 1 1> <1 1 1> 0.184 77.6
GaN (mp-804) <1 0 0> <1 1 0> 0.195 253.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.197 190.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.197 44.8
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.200 232.7
C (mp-48) <0 0 1> <1 0 0> 0.201 313.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
84 60 60 0 0 0
60 84 60 0 0 0
60 60 84 0 0 0
0 0 0 26 0 0
0 0 0 0 26 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
30.4 -12.7 -12.7 0 0 0
-12.7 30.4 -12.7 0 0 0
-12.7 -12.7 30.4 0 0 0
0 0 0 38.2 0 0
0 0 0 0 38.2 0
0 0 0 0 0 38.2
Shear Modulus GV
20 GPa
Bulk Modulus KV
68 GPa
Shear Modulus GR
17 GPa
Bulk Modulus KR
68 GPa
Shear Modulus GVRH
19 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
0.84
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrSi2 (mp-14172) 0.2546 0.003 2
SrSi2 (mp-496) 0.2612 0.003 2
BaSi2 (mp-7275) 0.1898 0.014 2
CaSiPt (mp-4478) 0.1592 0.000 3
SrSiPd (mp-8843) 0.3176 0.000 3
LaSiIr (mp-3555) 0.3172 0.000 3
SrSiPt (mp-971914) 0.3319 0.000 3
EuGePt (mp-19798) 0.2482 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ge_d Sr_sv Pt
Final Energy/Atom
-5.0238 eV
Corrected Energy
-60.2862 eV
-60.2862 eV = -60.2862 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 57115
Submitted by
User remarks:
  • High pressure experimental phase
  • Platinum strontium germanide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)