Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.313 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 0.005 | 47.8 |
ZrO2 (mp-2858) | <1 1 1> | <1 1 1> | 0.007 | 307.3 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 0.007 | 115.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 0.008 | 193.0 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 0.009 | 152.3 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 0.011 | 270.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.013 | 90.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 0.016 | 143.5 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 0.017 | 193.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 0.020 | 167.6 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 0.025 | 259.0 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 0.027 | 228.5 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 0.028 | 193.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 0.030 | 181.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 0.032 | 193.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 0.033 | 38.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 0.037 | 231.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 0.037 | 178.7 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 0.040 | 182.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 0.041 | 182.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 0.045 | 124.5 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 0.045 | 178.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 1 0> | 0.046 | 182.8 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 0.046 | 76.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 0.048 | 272.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 0.052 | 193.0 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 0.052 | 231.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 0.053 | 136.0 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 0.057 | 143.5 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 0.057 | 143.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 0.057 | 213.3 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 0.058 | 119.1 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 0.062 | 137.1 |
WS2 (mp-224) | <1 1 0> | <1 0 1> | 0.065 | 238.2 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 0.065 | 213.3 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 0.068 | 115.8 |
Ni (mp-23) | <1 1 1> | <1 1 0> | 0.069 | 191.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 0.069 | 213.3 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 0.070 | 317.4 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 0.070 | 193.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 0.071 | 91.4 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 0.071 | 193.0 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 0.075 | 152.3 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 0.075 | 91.4 |
Si (mp-149) | <1 1 0> | <1 0 1> | 0.076 | 297.8 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 0.077 | 198.0 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 0.078 | 136.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 0.083 | 77.2 |
TeO2 (mp-2125) | <1 0 1> | <1 1 1> | 0.083 | 307.3 |
GaP (mp-2490) | <1 1 0> | <1 0 1> | 0.084 | 297.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
103 | 71 | 65 | 0 | 0 | 0 |
71 | 85 | 55 | 0 | 0 | 0 |
65 | 55 | 99 | 0 | 0 | 0 |
0 | 0 | 0 | 7 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
26.3 | -16.9 | -7.9 | 0 | 0 | 0 |
-16.9 | 29.3 | -5.2 | 0 | 0 | 0 |
-7.9 | -5.2 | 18.1 | 0 | 0 | 0 |
0 | 0 | 0 | 135.2 | 0 | 0 |
0 | 0 | 0 | 0 | 69.8 | 0 |
0 | 0 | 0 | 0 | 0 | 41.7 |
Shear Modulus GV16 GPa |
Bulk Modulus KV74 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR72 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH73 GPa |
Elastic Anisotropy1.01 |
Poisson's Ratio0.41 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2Nb3Ge4 (mp-672696) | 0.6988 | 0.000 | 3 |
Hf2NiP (mp-5918) | 0.7030 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.6782 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.6513 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.3474 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.6236 | 0.106 | 4 |
ThNi (mp-623836) | 0.1826 | 0.000 | 2 |
PrAu (mp-999306) | 0.1939 | 0.006 | 2 |
CeAu (mp-1018087) | 0.1706 | 0.028 | 2 |
NdAu (mp-999338) | 0.2029 | 0.004 | 2 |
LaAu (mp-1002136) | 0.2003 | 0.000 | 2 |
Si (mp-1001113) | 0.5891 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Ni_pv |
Final Energy/Atom-6.1696 eV |
Corrected Energy-24.6785 eV
-24.6785 eV = -24.6785 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)