Final Magnetic Moment0.071 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.318 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYb2Ga + Yb2C3 + Yb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 198.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 322.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 140.2 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 171.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 198.2 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 171.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 297.3 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 214.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 175.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 123.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 171.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 123.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 272.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 105.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 123.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 173.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 140.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 272.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 105.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 198.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 300.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 280.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 280.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 123.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 198.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 105.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 322.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 140.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 171.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 123.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 140.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 272.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 148.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 371.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 105.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 223.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 70.1 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 140.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 173.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 214.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 297.3 |
Te2W (mp-22693) | <1 1 1> | <1 0 0> | 223.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 49.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 175.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 198.2 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 247.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 223.0 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 300.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 42.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
14 | 39 | 39 | 0 | 0 | 0 |
39 | 14 | 39 | 0 | 0 | 0 |
39 | 39 | 14 | 0 | 0 | 0 |
0 | 0 | 0 | 16 | 0 | 0 |
0 | 0 | 0 | 0 | 16 | 0 |
0 | 0 | 0 | 0 | 0 | 16 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-23.5 | 17.2 | 17.2 | 0 | 0 | 0 |
17.2 | -23.5 | 17.2 | 0 | 0 | 0 |
17.2 | 17.2 | -23.5 | 0 | 0 | 0 |
0 | 0 | 0 | 62.8 | 0 | 0 |
0 | 0 | 0 | 0 | 62.8 | 0 |
0 | 0 | 0 | 0 | 0 | 62.8 |
Shear Modulus GV5 GPa |
Bulk Modulus KV31 GPa |
Shear Modulus GR193 GPa |
Bulk Modulus KR31 GPa |
Shear Modulus GVRH99 GPa |
Bulk Modulus KVRH31 GPa |
Elastic Anisotropy-4.88 |
Poisson's Ratio-0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsCaO3 (mp-984240) | 0.0000 | 0.412 | 3 |
CaCuO3 (mp-1099873) | 0.0000 | 0.165 | 3 |
HgRhO3 (mp-1016877) | 0.0000 | 0.409 | 3 |
CdIrO3 (mp-1016828) | 0.0000 | 0.463 | 3 |
EuAgO3 (mp-1077622) | 0.0000 | 0.266 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.749 | 4 |
Fe4N (mp-535) | 0.0000 | 0.070 | 2 |
Sr3Sb2 (mp-1013583) | 0.0000 | 0.381 | 2 |
Ni4N (mp-20839) | 0.0000 | 2.021 | 2 |
Sr3P2 (mp-1013552) | 0.0000 | 0.403 | 2 |
Ca3P2 (mp-1013547) | 0.0000 | 0.145 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.247 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Ga_d C |
Final Energy/Atom-3.3080 eV |
Corrected Energy-16.5398 eV
Uncorrected energy = -16.5398 eV
Corrected energy = -16.5398 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)