Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.417 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmma [51] |
Hall-P 2a 2a |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 237.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 59.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 109.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 109.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 130.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 237.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 110.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 152.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 283.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 152.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 257.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 296.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 196.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 87.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 174.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 87.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 184.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 283.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 326.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 147.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 110.4 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 331.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 355.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 211.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 283.5 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 110.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 130.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 237.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 59.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 65.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 118.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 336.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 29.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 87.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 65.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 48.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 207.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 118.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 73.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 336.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 88.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 113.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 174.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 196.2 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 196.2 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 113.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 151.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 88.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 207.5 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 263.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NdInCo2 (mp-1078606) | 0.4060 | 0.054 | 3 |
HoInCo2 (mp-1079173) | 0.3538 | 0.044 | 3 |
NdInNi2 (mp-1079595) | 0.1349 | 0.000 | 3 |
YInCo2 (mp-1079716) | 0.4119 | 0.008 | 3 |
PrInNi2 (mp-1080775) | 0.1231 | 0.000 | 3 |
Lu7Te (mp-542388) | 0.6112 | 0.008 | 2 |
Mg4Si3 (mp-1074413) | 0.5638 | 0.252 | 2 |
Mg7Si4 (mp-1074856) | 0.6006 | 0.197 | 2 |
Mg3Si4 (mp-1075111) | 0.5111 | 0.256 | 2 |
Zr2Cu (mp-1077372) | 0.5830 | 0.057 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La In_d Ni_pv |
Final Energy/Atom-5.2285 eV |
Corrected Energy-41.8280 eV
-41.8280 eV = -41.8280 eV (uncorrected energy)
|