Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.695 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 283.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 204.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 170.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 122.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 218.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 194.4 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 187.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 263.0 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 265.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 163.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 47.2 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 230.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 159.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 218.7 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 172.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 218.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 121.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 24.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 121.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 131.5 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 81.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 94.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 263.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 263.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 286.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 315.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 164.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 267.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 194.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 286.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 218.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 159.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 194.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 94.4 |
BN (mp-984) | <1 0 0> | <1 0 1> | 212.3 |
BN (mp-984) | <1 0 1> | <1 0 0> | 141.6 |
BN (mp-984) | <1 1 0> | <0 1 1> | 204.4 |
BN (mp-984) | <1 1 1> | <0 1 1> | 204.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 131.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 163.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 47.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 170.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 65.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 286.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 230.1 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 1> | 265.4 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 159.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 218.7 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 265.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.3066 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.3205 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.3178 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.2984 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.5610 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.3255 | 0.106 | 4 |
GdGa (mp-20353) | 0.1502 | 0.000 | 2 |
SmGa (mp-999177) | 0.1667 | 0.000 | 2 |
GdGa (mp-917119) | 0.1491 | 0.000 | 2 |
NdGa (mp-1448) | 0.1841 | 0.000 | 2 |
TbGa (mp-11417) | 0.1783 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Si |
Final Energy/Atom-7.1135 eV |
Corrected Energy-56.9081 eV
-56.9081 eV = -56.9081 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)