Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.272 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.272 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToOs + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnnm [58] |
Hall-P 2 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 174.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 69.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 107.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 61.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 120.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 26.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 89.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 89.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 209.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 163.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 46.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 179.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 122.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 174.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 100.8 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 157.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 117.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 89.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 82.1 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 122.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 227.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 163.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 112.0 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 331.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 171.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 26.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 233.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 139.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 210.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 33.6 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 174.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 56.0 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 134.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 268.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.6 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 23.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 93.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 214.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 53.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 122.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 214.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 163.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 46.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 179.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 23.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 163.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 61.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 147.2 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 147.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
736 | 175 | 265 | 0 | 0 | 0 |
175 | 901 | 79 | 0 | 0 | 0 |
265 | 79 | 593 | 0 | 0 | 0 |
0 | 0 | 0 | 131 | 0 | 0 |
0 | 0 | 0 | 0 | 332 | 0 |
0 | 0 | 0 | 0 | 0 | 169 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
1.7 | -0.3 | -0.7 | 0 | 0 | 0.0 |
-0.3 | 1.2 | -0.0 | 0 | 0 | -0.0 |
-0.7 | -0.0 | 2.0 | 0 | 0 | -0.0 |
0 | 0 | 0 | 7.6 | 0 | 0 |
0 | 0 | 0 | 0 | 3.0 | 0 |
0.0 | -0.0 | -0.0 | 0 | 0 | 5.9 |
Shear Modulus GV240 GPa |
Bulk Modulus KV363 GPa |
Shear Modulus GR205 GPa |
Bulk Modulus KR355 GPa |
Shear Modulus GVRH223 GPa |
Bulk Modulus KVRH359 GPa |
Elastic Anisotropy0.89 |
Poisson's Ratio0.24 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba4Ta2O9 (mp-769394) | 0.6837 | 0.080 | 3 |
Sr4Ta2O9 (mp-769268) | 0.6443 | 0.032 | 3 |
Sr3WO6 (mp-769810) | 0.6933 | 0.000 | 3 |
Mg(HO)2 (mp-626143) | 0.6931 | 0.009 | 3 |
Mg2H2O3 (mp-30244) | 0.6879 | 0.020 | 3 |
Ca2TeWO6 (mvc-5060) | 0.7080 | 0.263 | 4 |
Na3Mo(OF)3 (mp-18753) | 0.6519 | 0.000 | 4 |
RhN2 (mp-20304) | 0.2734 | 0.098 | 2 |
RuN2 (mp-607371) | 0.0801 | 0.110 | 2 |
ReN2 (mp-1019077) | 0.5017 | 0.047 | 2 |
IrN2 (mp-13076) | 0.2207 | 0.200 | 2 |
FeN2 (mp-1080202) | 0.1382 | 0.137 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Os_pv N |
Final Energy/Atom-8.7717 eV |
Corrected Energy-52.6303 eV
-52.6303 eV = -52.6303 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)