material

TiCoSi

ID:

mp-21306

DOI:

10.17188/1196616


Tags: Titanium cobalt silicide (1/1/1) Cobalt titanium silicide (1/1/1) Cobalt silicon titanium (1/1/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.814 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 53079 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.018 272.3
Mg (mp-153) <1 0 1> <0 1 1> 0.038 170.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.040 136.2
C (mp-48) <1 0 0> <1 0 1> 0.051 95.9
Al2O3 (mp-1143) <1 0 1> <1 1 0> 0.053 197.4
YAlO3 (mp-3792) <0 1 1> <0 1 1> 0.054 239.1
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.063 143.8
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.082 363.1
TiO2 (mp-2657) <1 0 1> <0 1 1> 0.090 102.5
TePb (mp-19717) <1 0 0> <0 1 1> 0.091 170.8
KCl (mp-23193) <1 1 0> <0 1 0> 0.103 229.8
InAs (mp-20305) <1 0 0> <0 0 1> 0.111 113.5
CdWO4 (mp-19387) <1 1 0> <1 1 0> 0.115 246.7
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.125 126.6
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.131 113.5
Ni (mp-23) <1 1 0> <0 0 1> 0.158 158.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.168 249.6
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.170 170.8
SiC (mp-11714) <0 0 1> <0 0 1> 0.171 249.6
Ga2O3 (mp-886) <1 0 1> <0 1 1> 0.172 136.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.177 136.2
ZnO (mp-2133) <1 1 0> <0 1 0> 0.183 153.2
SiC (mp-8062) <1 0 0> <0 0 1> 0.191 113.5
Mg (mp-153) <1 0 0> <0 0 1> 0.192 181.5
Si (mp-149) <1 0 0> <1 0 1> 0.196 239.6
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.198 239.6
ZnO (mp-2133) <0 0 1> <0 1 0> 0.200 255.4
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.205 204.3
C (mp-48) <0 0 1> <0 0 1> 0.221 181.5
WS2 (mp-224) <1 1 1> <1 0 1> 0.223 239.6
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.226 246.7
SiC (mp-8062) <1 1 0> <0 0 1> 0.244 136.2
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.268 226.9
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.270 337.7
SiC (mp-11714) <1 1 1> <0 1 0> 0.280 332.0
SiO2 (mp-6930) <0 0 1> <0 1 0> 0.294 280.9
MgO (mp-1265) <1 1 1> <1 0 0> 0.296 126.6
GaP (mp-2490) <1 0 0> <1 0 1> 0.302 239.6
Te2W (mp-22693) <0 1 1> <0 1 0> 0.302 229.8
LiGaO2 (mp-5854) <0 1 0> <0 1 0> 0.313 332.0
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.313 204.3
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.315 204.3
Al (mp-134) <1 1 0> <0 1 0> 0.315 204.3
InAs (mp-20305) <1 1 0> <0 0 1> 0.346 158.8
TePb (mp-19717) <1 1 0> <0 1 1> 0.352 239.1
CdS (mp-672) <1 1 0> <1 1 0> 0.353 49.3
LiNbO3 (mp-3731) <0 0 1> <0 1 1> 0.355 239.1
Ni (mp-23) <1 1 1> <0 1 0> 0.362 280.9
GaTe (mp-542812) <0 0 1> <0 0 1> 0.363 226.9
CdSe (mp-2691) <1 0 0> <0 0 1> 0.371 113.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
285 112 115 0 0 0
112 313 149 0 0 0
115 149 283 0 0 0
0 0 0 114 0 0
0 0 0 0 123 0
0 0 0 0 0 103
Compliance Tensor Sij (10-12Pa-1)
4.4 -1 -1.3 0 0 0
-1 4.5 -2 0 0 0
-1.3 -2 5.1 0 0 0
0 0 0 8.8 0 0
0 0 0 0 8.1 0
0 0 0 0 0 9.7
Shear Modulus GV
102 GPa
Bulk Modulus KV
181 GPa
Shear Modulus GR
98 GPa
Bulk Modulus KR
180 GPa
Shear Modulus GVRH
100 GPa
Bulk Modulus KVRH
181 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HfCoAs (mp-9801) 0.2046 0.000 3
CaMgPb (mp-861738) 0.2063 0.000 3
HfFeP (mp-22434) 0.2347 0.000 3
ZrFeP (mp-20892) 0.2457 0.000 3
CaMgSn (mp-4864) 0.1919 0.000 3
Yb3In3Ge2Au (mp-981207) 0.5545 0.000 4
LiYb2InGe2 (mp-977355) 0.6292 0.000 4
K2BaCdSb2 (mp-863761) 0.5874 0.000 4
LiCa2InGe2 (mp-570850) 0.6217 0.000 4
U3Al3NiRu2 (mp-1080528) 0.6053 0.087 4
YbH2 (mp-864603) 0.2779 0.000 2
CaH2 (mp-23713) 0.3442 0.000 2
SrH2 (mp-23714) 0.3235 0.000 2
Co2P (mp-22204) 0.4115 0.000 2
BaH2 (mp-23715) 0.2996 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Co Si
Final Energy/Atom
-7.6228 eV
Corrected Energy
-91.1901 eV
Uncorrected energy = -91.4741 eV Composition-based energy adjustment (0.071 eV/atom x 4.0 atoms) = 0.2840 eV Corrected energy = -91.1901 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 165246
  • 625091
  • 53079
  • 625085
Submitted by
User remarks:
  • Titanium cobalt silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)