material

Te2Os

ID:

mp-2142

DOI:

10.17188/1196876


Tags: Osmium telluride Osmium telluride (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.072 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.523 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pa3 [205]
Hall
-P 2ac 2ab 3
Point Group
m3
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 24189 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 0 0> <1 0 0> 0.001 209.4
ZnO (mp-2133) <0 0 1> <1 1 1> 0.001 290.1
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.004 209.4
CdS (mp-672) <0 0 1> <1 1 1> 0.014 290.1
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.015 290.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.024 83.8
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.037 209.4
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.051 177.7
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.069 335.0
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.069 335.0
C (mp-66) <1 1 1> <1 1 1> 0.076 290.1
C (mp-66) <1 0 0> <1 0 0> 0.082 167.5
Ge (mp-32) <1 0 0> <1 0 0> 0.088 167.5
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.094 177.7
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.097 290.1
MgO (mp-1265) <1 1 1> <1 1 1> 0.098 217.6
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.189 145.1
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.199 209.4
GaAs (mp-2534) <1 0 0> <1 0 0> 0.199 167.5
CdS (mp-672) <1 1 1> <1 0 0> 0.205 209.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.239 118.4
Cu (mp-30) <1 1 1> <1 1 1> 0.245 290.1
Cu (mp-30) <1 0 0> <1 0 0> 0.264 167.5
C (mp-48) <0 0 1> <1 1 0> 0.277 236.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.290 167.5
CsI (mp-614603) <1 1 0> <1 1 0> 0.309 177.7
BN (mp-984) <1 0 1> <1 1 1> 0.330 217.6
SiC (mp-11714) <0 0 1> <1 1 0> 0.363 296.1
GaN (mp-804) <0 0 1> <1 1 0> 0.367 177.7
WS2 (mp-224) <0 0 1> <1 1 0> 0.374 177.7
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.375 177.7
SiC (mp-7631) <0 0 1> <1 1 0> 0.375 296.1
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.381 177.7
Ni (mp-23) <1 1 0> <1 0 0> 0.388 335.0
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.431 251.3
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.433 177.7
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.467 217.6
Mg (mp-153) <0 0 1> <1 1 0> 0.473 177.7
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.530 167.5
AlN (mp-661) <1 0 1> <1 1 0> 0.535 177.7
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.537 290.1
TiO2 (mp-390) <1 0 1> <1 1 0> 0.567 118.4
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.569 72.5
KCl (mp-23193) <1 1 1> <1 1 1> 0.593 72.5
SiC (mp-11714) <1 0 1> <1 0 0> 0.600 293.1
KCl (mp-23193) <1 1 0> <1 1 0> 0.604 59.2
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.616 145.1
KCl (mp-23193) <1 0 0> <1 0 0> 0.639 41.9
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.702 236.9
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.713 236.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
278 55 55 0 0 0
55 278 55 0 0 0
55 55 278 0 0 0
0 0 0 75 0 0
0 0 0 0 75 0
0 0 0 0 0 75
Compliance Tensor Sij (10-12Pa-1)
3.9 -0.6 -0.6 0 0 0
-0.6 3.9 -0.6 0 0 0
-0.6 -0.6 3.9 0 0 0
0 0 0 13.3 0 0
0 0 0 0 13.3 0
0 0 0 0 0 13.3
Shear Modulus GV
90 GPa
Bulk Modulus KV
129 GPa
Shear Modulus GR
87 GPa
Bulk Modulus KR
129 GPa
Shear Modulus GVRH
88 GPa
Bulk Modulus KVRH
129 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BiTePd (mp-29011) 0.1379 0.000 3
NiSbSe (mp-10847) 0.1677 0.000 3
SbTePd (mp-10850) 0.1065 0.000 3
BiTePt (mp-29638) 0.1450 0.000 3
SbIrSe (mp-1095507) 0.1787 0.000 3
Li3Ni(SbO3)4 (mp-849457) 0.5857 0.065 4
Mg2VWO6 (mvc-5881) 0.5670 0.018 4
Mg2MoWO6 (mvc-5910) 0.5888 0.031 4
Mg2CrWO6 (mvc-5960) 0.5588 0.047 4
InNi2SbO6 (mp-1078367) 0.5458 0.000 4
Sb2Pt (mp-562) 0.0875 0.000 2
CoSe2 (mp-22309) 0.0381 0.019 2
Sb2Pd (mp-1356) 0.0245 0.000 2
Te2Ru (mp-1848) 0.0120 0.006 2
Bi2Pt (mp-22864) 0.0754 0.009 2
Li4Fe2TeWO12 (mp-768021) 0.6958 0.083 5
Li4Mn2TeWO12 (mp-768044) 0.7457 0.054 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Te Os_pv
Final Energy/Atom
-5.9101 eV
Corrected Energy
-74.2975 eV
Uncorrected energy = -70.9215 eV Composition-based energy adjustment (-0.422 eV/atom x 8.0 atoms) = -3.3760 eV Corrected energy = -74.2975 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 300225
  • 24189
  • 647832
  • 647829
  • 647826
  • 647831
Submitted by
User remarks:
  • Osmium telluride (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)