material

YMgIn

ID:

mp-21503

DOI:

10.17188/1196957


Tags: Yttrium magnesium indium (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.414 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P62m [189]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 160910 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.001 197.5
Al (mp-134) <1 1 1> <0 0 1> 0.001 197.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.004 197.5
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.005 197.5
C (mp-48) <0 0 1> <0 0 1> 0.007 148.2
BN (mp-984) <0 0 1> <0 0 1> 0.007 49.4
AlN (mp-661) <1 0 0> <1 0 0> 0.008 141.6
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.011 283.2
Cu (mp-30) <1 1 0> <1 1 1> 0.011 314.9
InAs (mp-20305) <1 1 1> <0 0 1> 0.013 197.5
WS2 (mp-224) <0 0 1> <0 0 1> 0.014 345.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.015 345.7
SiC (mp-8062) <1 1 0> <1 0 1> 0.016 243.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.019 197.5
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.020 177.0
NaCl (mp-22862) <1 1 0> <1 0 1> 0.020 182.3
SiC (mp-7631) <1 1 0> <1 0 1> 0.022 243.0
Ni (mp-23) <1 1 1> <0 0 1> 0.025 148.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.026 197.5
BN (mp-984) <1 0 1> <1 0 1> 0.027 60.8
C (mp-66) <1 1 1> <0 0 1> 0.034 197.5
ZnO (mp-2133) <1 1 1> <1 0 0> 0.035 283.2
CdS (mp-672) <0 0 1> <0 0 1> 0.036 197.5
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.037 106.2
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.043 182.3
Mg (mp-153) <0 0 1> <0 0 1> 0.047 345.7
ZnO (mp-2133) <1 0 0> <0 0 1> 0.049 345.7
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.054 122.6
SiC (mp-7631) <1 0 0> <1 0 0> 0.064 141.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.069 148.2
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.071 177.0
LiGaO2 (mp-5854) <1 1 0> <1 0 1> 0.079 243.0
TiO2 (mp-390) <1 0 0> <0 0 1> 0.080 148.2
TiO2 (mp-390) <1 0 1> <1 0 0> 0.081 318.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.085 177.0
ZrO2 (mp-2858) <0 1 0> <1 0 1> 0.086 303.8
Al (mp-134) <1 1 0> <1 0 1> 0.088 182.3
AlN (mp-661) <1 1 0> <1 0 1> 0.091 243.0
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.108 303.8
SiC (mp-11714) <1 0 0> <1 0 0> 0.112 247.8
CdSe (mp-2691) <1 1 1> <0 0 1> 0.116 197.5
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.122 121.5
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.125 283.2
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.127 183.9
AlN (mp-661) <0 0 1> <1 0 0> 0.129 283.2
Ni (mp-23) <1 0 0> <1 0 0> 0.130 318.6
Te2W (mp-22693) <0 0 1> <1 1 0> 0.132 245.2
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.135 345.7
Ni (mp-23) <1 1 0> <0 0 1> 0.144 345.7
CdTe (mp-406) <1 1 0> <0 0 1> 0.146 246.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
98 26 35 0 0 0
26 98 35 0 0 0
35 35 97 0 0 0
0 0 0 52 0 0
0 0 0 0 52 0
0 0 0 0 0 36
Compliance Tensor Sij (10-12Pa-1)
12.1 -1.9 -3.7 0 0 0
-1.9 12.1 -3.7 0 0 0
-3.7 -3.7 13 0 0 0
0 0 0 19.4 0 0
0 0 0 0 19.4 0
0 0 0 0 0 28
Shear Modulus GV
41 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
39 GPa
Bulk Modulus KR
54 GPa
Shear Modulus GVRH
40 GPa
Bulk Modulus KVRH
54 GPa
Elastic Anisotropy
0.26
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SmMgIn (mp-21456) 0.0493 0.000 3
HoMgIn (mp-20538) 0.0350 0.000 3
DyMgIn (mp-20573) 0.0133 0.000 3
YMgAl (mp-13090) 0.0346 0.000 3
TmMgIn (mp-20979) 0.0639 0.000 3
Yb3In3Ge2Au (mp-981207) 0.3638 0.000 4
LiYb2InGe2 (mp-977355) 0.4647 0.000 4
Sr2LiInGe2 (mp-571617) 0.4273 0.000 4
LiCa2InGe2 (mp-570850) 0.4681 0.000 4
U3Al3NiRu2 (mp-1080528) 0.5460 0.087 4
Fe2P (mp-778) 0.5545 0.000 2
Pu2Co (mp-20026) 0.5848 0.060 2
CoSn3 (mp-985707) 0.6255 0.000 2
BaCl2 (mp-567680) 0.6420 0.030 2
CeSe2 (mp-1080312) 0.6036 0.012 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Mg_pv In_d
Final Energy/Atom
-4.0192 eV
Corrected Energy
-36.1724 eV
Uncorrected energy = -36.1724 eV Corrected energy = -36.1724 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 160910
Submitted by
User remarks:
  • Yttrium magnesium indium (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)