Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.458 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 0 1> | 250.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 167.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 322.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 286.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 250.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 322.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 214.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 250.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 250.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 181.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 143.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 358.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 286.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 322.2 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 272.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 214.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 286.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 179.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 195.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 250.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 107.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 214.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 322.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 322.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 322.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 286.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 143.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 292.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 250.6 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 250.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 250.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 286.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 286.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 214.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 179.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 358.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 141.3 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 195.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 358.0 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 250.6 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 250.6 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 250.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 107.4 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 322.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 179.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 97.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 250.6 |
C (mp-66) | <1 1 0> | <0 1 1> | 292.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 214.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 286.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce(In2Pd)2 (mp-641911) | 0.4232 | 0.002 | 3 |
Pr(In2Au)2 (mp-607514) | 0.1877 | 0.000 | 3 |
Nd(In2Au)2 (mp-607126) | 0.2402 | 0.009 | 3 |
Nd(Sn2Rh)2 (mp-669722) | 0.4881 | 0.000 | 3 |
Ce(In2Au)2 (mp-21537) | 0.1347 | 0.015 | 3 |
K2SrCdSb2 (mp-863758) | 0.6980 | 0.000 | 4 |
Mg2Si3 (mp-1073201) | 0.6794 | 0.252 | 2 |
Mg4Si3 (mp-1074465) | 0.6853 | 0.177 | 2 |
Mg3Si4 (mp-1074957) | 0.6820 | 0.189 | 2 |
Mg3Si4 (mp-1075018) | 0.6978 | 0.222 | 2 |
Mg3Si4 (mp-1075397) | 0.6498 | 0.334 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La In_d Au |
Final Energy/Atom-3.6714 eV |
Corrected Energy-102.7982 eV
Uncorrected energy = -102.7982 eV
Corrected energy = -102.7982 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)