Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.357 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 266.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 133.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 133.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 188.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 188.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 188.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 133.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 188.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 188.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 266.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 188.4 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 188.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 188.4 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 188.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 133.2 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 188.4 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 188.4 |
Si (mp-149) | <1 0 0> | <1 0 0> | 266.4 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 133.2 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 133.2 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 188.4 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 133.2 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 188.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg6Si7Ni16 (mp-570457) | 0.1287 | 0.000 | 3 |
Ti6Co16Si7 (mp-672677) | 0.0611 | 0.000 | 3 |
Ta6Si7Ni16 (mp-4502) | 0.1104 | 0.000 | 3 |
Nb6Ni16Ge7 (mp-672653) | 0.0690 | 0.013 | 3 |
Ta6Ni16Ge7 (mp-582719) | 0.0852 | 0.002 | 3 |
Zr6Co23 (mp-30569) | 0.3940 | 0.000 | 2 |
Zr6Fe23 (mp-582924) | 0.2965 | 0.007 | 2 |
Er6Zn23 (mp-30615) | 0.4010 | 0.010 | 2 |
Sr6Mg23 (mp-30782) | 0.3644 | 0.000 | 2 |
Er6Fe23 (mp-2162) | 0.3981 | 0.139 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ni_pv As |
Final Energy/Atom-5.0018 eV |
Corrected Energy-145.0516 eV
-145.0516 eV = -145.0516 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)