Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.388 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.040 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiAs2 + SiNi + SiNi2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 220.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 142.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 216.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 142.4 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 220.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 220.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 309.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 185.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 340.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 278.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 155.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 155.2 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 247.5 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 220.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 154.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 216.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.8 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 155.2 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 278.5 |
BN (mp-984) | <1 0 0> | <0 1 1> | 77.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 251.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 247.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 340.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 142.4 |
CdTe (mp-406) | <1 1 1> | <1 1 0> | 220.0 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 92.8 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 247.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 71.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 154.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 83.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 278.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 71.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 247.5 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 213.5 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 1> | 232.8 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 178.7 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 154.7 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 220.0 |
GaP (mp-2490) | <1 1 1> | <0 1 0> | 213.5 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 178.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 154.7 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 220.0 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 309.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 278.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 154.7 |
InSb (mp-20012) | <1 1 1> | <1 1 0> | 220.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 278.5 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 278.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni5Ge2P3 (mp-662818) | 0.3745 | 0.022 | 3 |
Si4MoPt3 (mp-978785) | 0.4732 | 0.000 | 3 |
Si2Ni5P3 (mp-649521) | 0.3471 | 0.051 | 3 |
Ni2GeP (mp-618929) | 0.4339 | 0.022 | 3 |
SiNi2P (mp-510422) | 0.3002 | 0.022 | 3 |
TiTlCuTe3 (mp-9344) | 0.7116 | 0.000 | 4 |
RbHfAgTe3 (mp-9780) | 0.6991 | 0.000 | 4 |
ZrSb2 (mp-979) | 0.6118 | 0.000 | 2 |
HfSb2 (mp-2180) | 0.5575 | 0.000 | 2 |
ZrBi2 (mp-29642) | 0.5294 | 0.000 | 2 |
Mg4Si3 (mp-1078478) | 0.4858 | 0.260 | 2 |
CrBi (mp-1079128) | 0.6029 | 0.609 | 2 |
Bi (mp-1067758) | 0.6957 | 0.086 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Ni_pv As |
Final Energy/Atom-5.7990 eV |
Corrected Energy-185.5665 eV
-185.5665 eV = -185.5665 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)