@article{Zaremba2001, author = "Zaremba, V. and Muts, I. and Kal'ichak, Ya.M. and Hoffmann, R.D. and Poettgen, R.", title = "Ca3 Ni8 In4 - An ordered non-centrosymmetric variant of the Ba Li4 type", journal = "Journal of Solid State Chemistry", year = "2001", volume = "160", pages = "415-420", ASTM_id = "JSSCBI" }