material

Li2Pt

ID:

mp-2170

DOI:

10.17188/1197123


Tags: Lithium platinum (2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.542 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 104780 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.000 60.0
Ge (mp-32) <1 1 0> <1 1 0> 0.001 235.3
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.007 172.8
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.008 270.1
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.010 156.8
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.010 156.8
Cu (mp-30) <1 1 0> <1 1 1> 0.011 74.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.013 195.1
BaF2 (mp-1029) <1 1 0> <1 1 1> 0.015 222.2
AlN (mp-661) <1 1 0> <1 0 0> 0.016 135.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.017 235.3
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.018 137.2
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.022 124.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.025 285.1
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.026 195.1
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.028 105.0
C (mp-48) <1 0 0> <1 0 0> 0.029 192.4
LaF3 (mp-905) <0 0 1> <0 0 1> 0.030 45.0
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.031 225.1
GaTe (mp-542812) <1 0 0> <1 0 0> 0.031 45.3
GaTe (mp-542812) <0 0 1> <1 0 1> 0.033 75.2
CdS (mp-672) <1 1 1> <1 1 0> 0.033 156.8
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.033 195.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.034 235.3
BN (mp-984) <0 0 1> <0 0 1> 0.036 105.0
AlN (mp-661) <0 0 1> <0 0 1> 0.038 60.0
BN (mp-984) <1 0 0> <1 0 0> 0.039 135.8
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.040 156.8
SiO2 (mp-6930) <1 0 1> <1 0 1> 0.044 244.3
CdS (mp-672) <1 1 0> <1 1 1> 0.045 49.4
TiO2 (mp-390) <1 1 1> <1 0 0> 0.048 215.1
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.053 181.1
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.056 15.0
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.058 176.4
KCl (mp-23193) <1 0 0> <1 0 1> 0.060 206.8
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.061 169.8
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.065 135.8
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.069 45.3
InP (mp-20351) <1 1 0> <1 0 1> 0.071 150.4
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.071 169.8
PbSe (mp-2201) <1 1 0> <1 1 1> 0.073 222.2
LiNbO3 (mp-3731) <1 1 1> <1 0 1> 0.073 131.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.077 158.5
CaCO3 (mp-3953) <1 0 0> <1 0 0> 0.078 260.3
InAs (mp-20305) <1 1 1> <0 0 1> 0.092 195.1
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.095 176.4
Si (mp-149) <1 0 0> <1 0 0> 0.096 90.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.096 215.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.097 90.6
GaSb (mp-1156) <1 1 0> <1 1 1> 0.097 222.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
100 36 36 0 0 0
36 100 36 0 0 0
36 36 234 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
11.9 -3.8 -1.3 0 0 0
-3.8 11.9 -1.3 0 0 0
-1.3 -1.3 4.7 0 0 0
0 0 0 56.7 0 0
0 0 0 0 56.7 0
0 0 0 0 0 31.4
Shear Modulus GV
35 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
64 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
1.84
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiAlPt (mp-1025063) 0.0369 0.102 3
MnNiGe (mp-21090) 0.0771 0.032 3
MnNiGe (mp-583202) 0.0736 0.323 3
TiAlAu (mp-16481) 0.0771 0.000 3
LiSnAu (mp-11977) 0.0926 0.001 3
Li2Pd (mp-728) 0.0771 0.000 2
Yb2Sn (mp-570050) 0.0468 0.000 2
Mg2Si (mp-1018796) 0.0346 0.160 2
Mg2Ge (mp-1018794) 0.1119 0.153 2
ThCd2 (mp-1210) 0.0318 0.000 2
Ti (mp-72) 0.4209 0.000 1
Li (mp-1063005) 0.7281 0.019 1
Hf (mp-1009460) 0.4316 0.045 1
Hg (mp-10861) 0.7027 0.003 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Pt
Final Energy/Atom
-3.8385 eV
Corrected Energy
-11.5155 eV
-11.5155 eV = -11.5155 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104780
  • 642278
Submitted by
User remarks:
  • Lithium platinum (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)