Final Magnetic Moment0.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.413 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.781 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 1 1> | <0 0 1> | 106.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 212.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 212.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 212.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 212.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 234.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 1> | 158.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 106.5 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 212.9 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 117.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 158.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 212.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 106.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 234.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 212.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 117.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 234.8 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 234.8 |
C (mp-48) | <0 0 1> | <1 0 1> | 158.6 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 117.4 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 234.8 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 106.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Al2As3 (mp-17473) | 0.3801 | 0.000 | 3 |
Rb2In2Sb3 (mp-21760) | 0.3253 | 0.000 | 3 |
K2In2Sb3 (mp-579637) | 0.3491 | 0.000 | 3 |
Na2Ga2As3 (mp-15431) | 0.2826 | 0.000 | 3 |
K2Ga2As3 (mp-15432) | 0.3630 | 0.000 | 3 |
BaLi4NiO4 (mp-776790) | 0.6119 | 0.105 | 4 |
K2Li3MnO4 (mp-773442) | 0.6483 | 0.174 | 4 |
K3Na2InO4 (mp-553975) | 0.6326 | 0.000 | 4 |
LiCaAlN2 (mp-1020031) | 0.5654 | 0.000 | 4 |
K2Na3InO4 (mp-504962) | 0.6436 | 0.000 | 4 |
MgSi2 (mp-1073528) | 0.6085 | 0.150 | 2 |
Mg3Si4 (mp-1075152) | 0.5817 | 0.150 | 2 |
Mg3Si4 (mp-1075355) | 0.6437 | 0.191 | 2 |
Mg5Si6 (mp-1075403) | 0.6177 | 0.201 | 2 |
Mg5Si9 (mp-1075724) | 0.6094 | 0.253 | 2 |
Si (mp-676011) | 0.7409 | 0.445 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv In_d As |
Final Energy/Atom-3.5126 eV |
Corrected Energy-196.7042 eV
Uncorrected energy = -196.7042 eV
Corrected energy = -196.7042 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)