Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.398 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 288.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 219.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 68.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 77.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 107.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 184.8 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 219.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 41.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 50.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 204.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 123.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 126.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 126.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 336.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 219.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 38.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 55.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 67.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 38.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 55.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 67.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 117.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 123.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 96.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 123.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 126.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 67.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 165.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 110.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 247.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 155.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 123.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 261.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 316.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 340.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 126.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 282.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 38.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 55.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 67.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 126.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 336.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 219.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 77.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 247.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 117.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 175.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 262.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 301.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 262.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
353 | 171 | 171 | 0 | 0 | 0 |
171 | 353 | 171 | 0 | 0 | 0 |
171 | 171 | 353 | 0 | 0 | 0 |
0 | 0 | 0 | 61 | 0 | 0 |
0 | 0 | 0 | 0 | 61 | 0 |
0 | 0 | 0 | 0 | 0 | 61 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.1 | -1.4 | -1.4 | 0 | 0 | 0 |
-1.4 | 4.1 | -1.4 | 0 | 0 | 0 |
-1.4 | -1.4 | 4.1 | 0 | 0 | 0 |
0 | 0 | 0 | 16.5 | 0 | 0 |
0 | 0 | 0 | 0 | 16.5 | 0 |
0 | 0 | 0 | 0 | 0 | 16.5 |
Shear Modulus GV73 GPa |
Bulk Modulus KV232 GPa |
Shear Modulus GR70 GPa |
Bulk Modulus KR232 GPa |
Shear Modulus GVRH71 GPa |
Bulk Modulus KVRH232 GPa |
Elastic Anisotropy0.20 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.063 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.007 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.228 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Re_pv |
Final Energy/Atom-10.5679 eV |
Corrected Energy-21.1359 eV
-21.1359 eV = -21.1359 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)