Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.549 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 250.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 318.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 212.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 318.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 282.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 306.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 183.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 176.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 250.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 282.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 318.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 245.0 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 306.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 300.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 200.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 141.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 282.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 245.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 70.7 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 306.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 183.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 176.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 318.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 318.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 282.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 141.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 200.1 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 61.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 35.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 318.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 176.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 282.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 176.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 200.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 300.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 61.3 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 61.3 |
Al (mp-134) | <1 1 0> | <1 1 0> | 200.1 |
Al (mp-134) | <1 1 1> | <1 1 1> | 245.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 306.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 212.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 176.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 50.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 176.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 353.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 176.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 70.7 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 100.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 35.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 176.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
243 | 26 | 26 | 0 | 0 | 0 |
26 | 243 | 26 | 0 | 0 | 0 |
26 | 26 | 243 | 0 | 0 | 0 |
0 | 0 | 0 | 3 | 0 | 0 |
0 | 0 | 0 | 0 | 3 | 0 |
0 | 0 | 0 | 0 | 0 | 3 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.2 | -0.4 | -0.4 | 0 | 0 | 0 |
-0.4 | 4.2 | -0.4 | 0 | 0 | 0 |
-0.4 | -0.4 | 4.2 | 0 | 0 | 0 |
0 | 0 | 0 | 311.7 | 0 | 0 |
0 | 0 | 0 | 0 | 311.7 | 0 |
0 | 0 | 0 | 0 | 0 | 311.7 |
Shear Modulus GV45 GPa |
Bulk Modulus KV98 GPa |
Shear Modulus GR5 GPa |
Bulk Modulus KR98 GPa |
Shear Modulus GVRH25 GPa |
Bulk Modulus KVRH98 GPa |
Elastic Anisotropy38.30 |
Poisson's Ratio0.38 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.039 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
LuSe (mp-414) | 0.0000 | 0.000 | 2 |
PrP (mp-601) | 0.0000 | 0.000 | 2 |
BeO (mp-1794) | 0.0000 | 0.481 | 2 |
HoAs (mp-295) | 0.0000 | 0.000 | 2 |
PtN (mp-13175) | 0.0000 | 1.193 | 2 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.393 | 1 |
C (mp-998866) | 0.0000 | 2.763 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Na (mp-1093989) | 0.0000 | 1.074 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Se |
Final Energy/Atom-7.0043 eV |
Corrected Energy-14.0085 eV
-14.0085 eV = -14.0085 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)