Final Magnetic Moment0.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.354 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.788 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 125.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 251.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 125.9 |
BN (mp-984) | <1 0 0> | <1 0 1> | 191.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 191.9 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 251.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 251.8 |
C (mp-66) | <1 0 0> | <1 0 1> | 191.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 125.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 251.8 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 251.8 |
Si (mp-149) | <1 1 0> | <0 0 1> | 125.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 125.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 125.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 251.8 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 191.9 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 251.8 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 125.9 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 125.9 |
C (mp-48) | <1 0 0> | <1 0 1> | 191.9 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 251.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 251.8 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 125.9 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 125.9 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 125.9 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 125.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2In2Sb3 (mp-21760) | 0.2435 | 0.000 | 3 |
K2Al2Sb3 (mp-17886) | 0.2262 | 0.000 | 3 |
K2In2Sb3 (mp-579637) | 0.4061 | 0.000 | 3 |
K2Ga2As3 (mp-15432) | 0.1579 | 0.000 | 3 |
K2Ga2Sb3 (mp-15433) | 0.2249 | 0.000 | 3 |
KLiNiO2 (mp-776912) | 0.7116 | 0.058 | 4 |
Ba2Li3NbN4 (mp-567658) | 0.6752 | 0.014 | 4 |
Ba2Li3TaN4 (mp-573677) | 0.6866 | 0.008 | 4 |
Ho3CuSnS7 (mp-554553) | 0.7020 | 0.019 | 4 |
EuCu2SnS4 (mp-555984) | 0.6776 | 0.035 | 4 |
MgSi2 (mp-1073528) | 0.6184 | 0.150 | 2 |
MgSi2 (mp-1073539) | 0.7475 | 0.182 | 2 |
Mg5Si6 (mp-1075403) | 0.7305 | 0.201 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv In_d Sb |
Final Energy/Atom-3.1658 eV |
Corrected Energy-181.8922 eV
Uncorrected energy = -177.2842 eV
Composition-based energy adjustment (-0.192 eV/atom x 24.0 atoms) = -4.6080 eV
Corrected energy = -181.8922 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)