material

NiAs2

ID:

mp-21873

DOI:

10.17188/1197216


Tags: Nickel arsenide (1/2) Krutovite Nickel arsenide (1/2) - HP

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.240 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.018 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.15 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NiAs2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pa3 [205]
Hall
-P 2ac 2ab 3
Point Group
m3
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 42569 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <1 1 1> 0.000 58.0
SiC (mp-7631) <0 0 1> <1 1 1> 0.001 58.0
SiC (mp-8062) <1 1 1> <1 1 1> 0.003 232.0
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.007 94.7
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.008 67.0
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.012 267.9
LiF (mp-1138) <1 1 0> <1 1 0> 0.012 47.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.013 33.5
Si (mp-149) <1 0 0> <1 0 0> 0.015 267.9
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.020 267.9
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.021 94.7
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.035 134.0
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.036 167.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.045 174.0
MgO (mp-1265) <1 1 0> <1 1 0> 0.045 284.2
Ge (mp-32) <1 1 1> <1 1 1> 0.046 58.0
Ge (mp-32) <1 1 0> <1 1 0> 0.047 47.4
C (mp-66) <1 0 0> <1 0 0> 0.047 167.5
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.051 142.1
Ge (mp-32) <1 0 0> <1 0 0> 0.051 33.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.052 167.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.055 94.7
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.055 234.4
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.077 142.1
GaAs (mp-2534) <1 1 1> <1 1 1> 0.105 58.0
GaAs (mp-2534) <1 1 0> <1 1 0> 0.108 47.4
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.110 167.5
GaAs (mp-2534) <1 0 0> <1 0 0> 0.118 33.5
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.121 94.7
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.126 267.9
InSb (mp-20012) <1 1 1> <1 1 1> 0.140 232.0
InSb (mp-20012) <1 1 0> <1 1 0> 0.143 189.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.144 301.4
AlN (mp-661) <0 0 1> <1 1 0> 0.154 236.8
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.154 58.0
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.155 301.4
GaSe (mp-1943) <0 0 1> <1 1 0> 0.156 189.5
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.158 47.4
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.161 301.4
CdTe (mp-406) <1 1 1> <1 1 1> 0.164 232.0
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.167 301.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.168 189.5
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.173 33.5
WS2 (mp-224) <1 1 0> <1 1 1> 0.175 232.0
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.189 267.9
Mg (mp-153) <1 1 1> <1 0 0> 0.192 267.9
LiF (mp-1138) <1 1 1> <1 0 0> 0.193 234.4
C (mp-66) <1 1 0> <1 1 0> 0.200 142.1
GaN (mp-804) <0 0 1> <1 0 0> 0.201 334.9
BN (mp-984) <0 0 1> <1 1 0> 0.203 189.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
230 54 54 0 0 0
54 230 54 0 0 0
54 54 230 0 0 0
0 0 0 38 0 0
0 0 0 0 38 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
4.8 -0.9 -0.9 0 0 0
-0.9 4.8 -0.9 0 0 0
-0.9 -0.9 4.8 0 0 0
0 0 0 26.1 0 0
0 0 0 0 26.1 0
0 0 0 0 0 26.1
Shear Modulus GV
58 GPa
Bulk Modulus KV
113 GPa
Shear Modulus GR
49 GPa
Bulk Modulus KR
113 GPa
Shear Modulus GVRH
54 GPa
Bulk Modulus KVRH
113 GPa
Elastic Anisotropy
0.87
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CoAsS (mp-16363) 0.1389 0.004 3
NiAsSe (mp-10846) 0.1004 0.000 3
SbTePd (mp-10850) 0.1530 0.000 3
SbIrSe (mp-1095507) 0.1071 0.000 3
SbPdSe (mp-4368) 0.1293 0.000 3
Li2VSi3O8 (mp-767616) 0.6080 0.092 4
Li2Co3SnO8 (mp-765424) 0.6258 0.214 4
Li2Si3NiO8 (mp-767953) 0.6183 0.076 4
InNi2SbO6 (mp-1078367) 0.6194 0.000 4
CuAsPtS2 (mp-1078511) 0.6029 0.000 4
Sb2Au (mp-738) 0.0140 0.011 2
Sb2Pt (mp-562) 0.0578 0.000 2
RhSe2 (mp-983) 0.0385 0.034 2
OsSe2 (mp-2480) 0.0266 0.000 2
NiSe2 (mp-20901) 0.0075 0.014 2
Li4Ti3Mn3(NiO8)2 (mp-770507) 0.7448 0.061 5
Li4Fe3Co2Cu3O16 (mp-763163) 0.7322 0.090 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv As
Final Energy/Atom
-5.2726 eV
Corrected Energy
-63.2708 eV
Uncorrected energy = -63.2708 eV Corrected energy = -63.2708 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 42569
  • 611031
Submitted by
User remarks:
  • Krutovite
  • Nickel arsenide (1/2) - HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)