Final Magnetic Moment0.832 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.428 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCe(NiSn)2 |
Band Gap0.001 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 204.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 294.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 68.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 294.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 230.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 215.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 215.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 157.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 157.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 294.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 200.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 272.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 230.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 176.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 98.1 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 136.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 294.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 157.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 157.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 276.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 255.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 196.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 157.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 250.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 314.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 250.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.3 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 272.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 300.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 314.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 255.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 65.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 294.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 157.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 300.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 65.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 322.7 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 195.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 322.7 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 195.6 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 195.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 137.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 136.2 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 65.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba(SbPd)2 (mp-6963) | 0.0115 | 0.017 | 3 |
Nd(SiRu)2 (mp-4013) | 0.0554 | 0.000 | 3 |
Pr(GeRu)2 (mp-569607) | 0.0653 | 0.000 | 3 |
La(GeRu)2 (mp-19900) | 0.0342 | 0.000 | 3 |
Pr(SiRu)2 (mp-4904) | 0.0395 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.5838 | 0.000 | 4 |
EuGa4 (mp-21884) | 0.4394 | 0.000 | 2 |
ThZn4 (mp-536) | 0.4250 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.4374 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.4424 | 0.000 | 2 |
BaGa4 (mp-335) | 0.3566 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv Sn_d Ce |
Final Energy/Atom-5.5309 eV |
Corrected Energy-27.6544 eV
-27.6544 eV = -27.6544 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)