material

ZrSbPd

ID:

mp-22036

DOI:

10.17188/1197305


Tags: Zirconium palladium antimonide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.748 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zr3Sb7Pd + ZrSb + ZrPd3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 92441 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 1 0> 0.001 174.8
CdS (mp-672) <1 0 0> <0 1 1> 0.009 230.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.010 239.3
GaN (mp-804) <1 1 0> <0 1 0> 0.015 174.8
GdScO3 (mp-5690) <1 0 0> <0 1 0> 0.016 139.9
CdS (mp-672) <1 1 0> <0 0 1> 0.023 149.6
Al2O3 (mp-1143) <1 0 0> <0 1 0> 0.025 314.7
TeO2 (mp-2125) <1 1 0> <1 1 0> 0.031 196.4
C (mp-48) <1 0 1> <0 1 0> 0.035 139.9
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.038 314.6
SiC (mp-8062) <1 1 1> <0 0 1> 0.039 299.1
KCl (mp-23193) <1 0 0> <1 1 0> 0.040 327.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.040 269.2
Cu (mp-30) <1 0 0> <1 1 0> 0.040 65.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.041 149.6
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.043 261.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.043 149.6
Ni (mp-23) <1 0 0> <0 1 1> 0.047 184.1
Al (mp-134) <1 0 0> <1 1 0> 0.047 65.5
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.047 131.0
AlN (mp-661) <1 0 1> <1 1 0> 0.047 196.4
ZrO2 (mp-2858) <1 0 0> <0 1 1> 0.049 230.1
TiO2 (mp-390) <0 0 1> <1 1 0> 0.052 131.0
CdS (mp-672) <1 1 1> <1 1 0> 0.057 261.9
CdWO4 (mp-19387) <0 1 1> <0 1 0> 0.061 244.8
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.064 131.0
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.065 119.7
ZnO (mp-2133) <1 0 1> <0 1 0> 0.068 314.7
GaSe (mp-1943) <0 0 1> <1 1 1> 0.070 288.0
Mg (mp-153) <1 1 0> <0 1 0> 0.071 174.8
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.080 65.5
ZnSe (mp-1190) <1 1 0> <0 1 0> 0.081 139.9
KP(HO2)2 (mp-23959) <1 0 0> <0 1 1> 0.085 230.1
AlN (mp-661) <1 1 1> <0 1 1> 0.088 230.1
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.091 209.4
KP(HO2)2 (mp-23959) <1 0 1> <0 1 1> 0.092 138.1
ZnSe (mp-1190) <1 0 0> <1 1 0> 0.093 65.5
GaAs (mp-2534) <1 1 0> <0 1 0> 0.094 139.9
ZnO (mp-2133) <0 0 1> <0 1 0> 0.103 349.7
C (mp-48) <1 0 0> <0 0 1> 0.115 209.4
TbScO3 (mp-31119) <1 0 0> <0 1 0> 0.117 139.9
TeO2 (mp-2125) <0 1 1> <0 1 1> 0.120 230.1
NaCl (mp-22862) <1 0 0> <1 1 0> 0.125 65.5
ZnO (mp-2133) <1 0 0> <0 1 1> 0.126 138.1
C (mp-66) <1 1 0> <0 1 1> 0.127 322.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.127 299.1
SiC (mp-11714) <1 1 0> <0 1 1> 0.136 322.1
GaAs (mp-2534) <1 0 0> <1 1 0> 0.137 65.5
Ge (mp-32) <1 1 0> <0 1 0> 0.145 139.9
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.147 251.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
167 85 114 0 0 0
85 198 112 0 0 0
114 112 174 0 0 0
0 0 0 52 0 0
0 0 0 0 34 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
11 -1 -6.5 0 0 0
-1 8.1 -4.6 0 0 0
-6.5 -4.6 13 0 0 0
0 0 0 19.1 0 0
0 0 0 0 29.8 0
0 0 0 0 0 37.3
Shear Modulus GV
38 GPa
Bulk Modulus KV
129 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
128 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
128 GPa
Elastic Anisotropy
0.47
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HfCuSi (mp-22489) 0.3235 0.000 3
LuGeIr (mp-10999) 0.3122 0.000 3
YbZnPd (mp-13025) 0.3168 0.000 3
ScGeRh (mp-1095247) 0.3177 0.005 3
HfCuGe (mp-1095504) 0.1554 0.018 3
Na2LiGaAs2 (mp-9722) 0.6378 0.000 4
Na2LiAlP2 (mp-9719) 0.6834 0.000 4
K2LiGaAs2 (mp-9703) 0.6961 0.000 4
KNa4SnSb3 (mp-6758) 0.6285 0.005 4
K2LiInAs2 (mp-505431) 0.6647 0.000 4
Sr2Sn (mp-978) 0.4701 0.000 2
Ca2Pb (mp-30478) 0.4214 0.000 2
Yb2Ge (mp-1694) 0.4527 0.000 2
Ca2Sn (mp-22735) 0.4224 0.000 2
Eu2Ge (mp-1095642) 0.4692 0.000 2
Rb (mp-640416) 0.7352 0.057 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Sb Pd
Final Energy/Atom
-6.7004 eV
Corrected Energy
-80.4053 eV
Uncorrected energy = -80.4053 eV Corrected energy = -80.4053 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 92441
Submitted by
User remarks:
  • Zirconium palladium antimonide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)