material

Ta2InC

ID:

mp-22144

DOI:

10.17188/1197373


Tags: High pressure experimental phase Tantalum indium carbide (2/1/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.377 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.071 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ta2C + In
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.000 60.8
Al (mp-134) <1 1 1> <0 0 1> 0.000 113.0
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.003 165.1
Te2W (mp-22693) <0 0 1> <0 0 1> 0.007 243.3
PbSe (mp-2201) <1 1 1> <0 0 1> 0.007 269.4
LaF3 (mp-905) <1 0 0> <1 0 0> 0.011 322.2
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.012 113.0
BN (mp-984) <0 0 1> <0 0 1> 0.015 104.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.015 165.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.022 113.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.027 269.4
GaSe (mp-1943) <0 0 1> <0 0 1> 0.031 113.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.044 182.5
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.045 139.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.051 269.4
CdS (mp-672) <0 0 1> <0 0 1> 0.060 60.8
Mg (mp-153) <1 0 0> <1 0 0> 0.062 184.1
Mg (mp-153) <1 1 0> <0 0 1> 0.065 86.9
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.067 338.9
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.072 208.5
Si (mp-149) <1 0 0> <0 0 1> 0.076 208.5
Mg (mp-153) <0 0 1> <0 0 1> 0.105 8.7
InP (mp-20351) <1 1 1> <0 0 1> 0.108 60.8
WS2 (mp-224) <1 1 1> <0 0 1> 0.111 78.2
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.116 156.4
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.123 276.2
MgO (mp-1265) <1 1 1> <0 0 1> 0.125 217.2
Ga2O3 (mp-886) <1 1 1> <0 0 1> 0.127 252.0
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.132 139.0
GaTe (mp-542812) <0 0 1> <0 0 1> 0.133 304.1
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.144 234.2
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.171 156.4
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.182 139.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.187 60.8
C (mp-66) <1 1 1> <0 0 1> 0.194 269.4
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.195 52.1
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.199 139.0
LaF3 (mp-905) <1 1 0> <0 0 1> 0.212 278.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.212 8.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.214 8.7
KCl (mp-23193) <1 1 0> <0 0 1> 0.226 173.8
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.226 269.4
Cu (mp-30) <1 1 0> <0 0 1> 0.228 278.0
MoS2 (mp-1434) <1 0 1> <1 0 0> 0.230 138.1
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.240 138.1
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.256 269.4
InSb (mp-20012) <1 1 0> <0 0 1> 0.257 312.8
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.260 86.9
CdTe (mp-406) <1 1 0> <0 0 1> 0.271 312.8
BN (mp-984) <1 1 0> <0 0 1> 0.277 269.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
311 90 126 0 0 0
90 311 126 0 0 0
126 126 291 0 0 0
0 0 0 105 0 0
0 0 0 0 105 0
0 0 0 0 0 111
Compliance Tensor Sij (10-12Pa-1)
4 -0.5 -1.5 0 0 0
-0.5 4 -1.5 0 0 0
-1.5 -1.5 4.7 0 0 0
0 0 0 9.5 0 0
0 0 0 0 9.5 0
0 0 0 0 0 9
Shear Modulus GV
102 GPa
Bulk Modulus KV
177 GPa
Shear Modulus GR
101 GPa
Bulk Modulus KR
177 GPa
Shear Modulus GVRH
102 GPa
Bulk Modulus KVRH
177 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zr2InC (mp-20004) 0.1057 0.000 3
Hf2InC (mp-22156) 0.1026 0.000 3
Sc2AlC (mp-13070) 0.0182 0.100 3
Nb2InC (mp-19835) 0.0550 0.000 3
Ti2AlN (mp-4978) 0.1095 0.000 3
Co3H (mp-1025425) 0.2247 0.182 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ta_pv In_d C
Final Energy/Atom
-9.3003 eV
Corrected Energy
-74.4027 eV
-74.4027 eV = -74.4027 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 163523
  • 163522
  • 163509
Submitted by
User remarks:
  • High pressure experimental phase
  • Tantalum indium carbide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)