Final Magnetic Moment
0.069 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.283 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.79 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 163143 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <0 0 1> 0.000 138.6
Ni (mp-23) <1 0 0> <0 0 1> 0.000 61.6
Ag (mp-124) <1 1 0> <1 0 0> 0.001 244.3
CdSe (mp-2691) <1 0 0> <0 0 1> 0.004 77.0
CsI (mp-614603) <1 0 0> <0 0 1> 0.004 61.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.005 77.0
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.005 289.5
Au (mp-81) <1 0 0> <0 0 1> 0.009 138.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.010 77.0
GaN (mp-804) <0 0 1> <0 0 1> 0.013 169.3
Au (mp-81) <1 1 0> <1 0 0> 0.014 244.3
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.016 77.0
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.020 30.8
InAs (mp-20305) <1 0 0> <0 0 1> 0.022 77.0
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.023 138.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.023 77.0
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.024 61.6
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.028 76.8
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.033 215.5
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.034 192.0
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.035 268.7
GdScO3 (mp-5690) <0 1 1> <1 1 1> 0.037 165.5
SrTiO3 (mp-4651) <1 1 1> <1 0 1> 0.037 280.9
WSe2 (mp-1821) <1 0 0> <1 1 1> 0.039 248.2
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.042 108.6
GaP (mp-2490) <1 1 0> <0 0 1> 0.043 215.5
Mg (mp-153) <1 1 0> <1 1 0> 0.046 115.2
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.049 124.1
Te2W (mp-22693) <0 1 1> <1 1 0> 0.050 115.2
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.050 277.1
SiO2 (mp-6930) <1 0 0> <1 1 1> 0.051 82.7
BN (mp-984) <1 0 1> <0 0 1> 0.054 200.1
GaN (mp-804) <1 1 0> <1 1 0> 0.054 115.2
CdWO4 (mp-19387) <1 1 1> <1 1 0> 0.055 153.6
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.056 61.6
SiC (mp-11714) <0 0 1> <1 1 0> 0.057 307.1
SiC (mp-7631) <0 0 1> <1 1 0> 0.058 307.1
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.059 30.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.071 138.6
Ga2O3 (mp-886) <0 1 0> <1 0 1> 0.071 280.9
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.074 217.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.074 230.9
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.075 190.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.078 323.3
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.082 271.5
CdS (mp-672) <1 0 0> <1 1 0> 0.083 115.2
GaN (mp-804) <1 1 1> <1 1 0> 0.095 153.6
GaP (mp-2490) <1 0 0> <0 0 1> 0.099 30.8
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.102 292.5
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.112 307.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
117 37 30 0 0 0
37 117 30 0 0 0
30 30 56 0 0 0
0 0 0 27 0 0
0 0 0 0 27 0
0 0 0 0 0 56
Compliance Tensor Sij (10-12Pa-1)
10.4 -2.1 -4.5 0 0 0
-2.1 10.4 -4.5 0 0 0
-4.5 -4.5 23 0 0 0
0 0 0 37.2 0 0
0 0 0 0 37.2 0
0 0 0 0 0 17.9
Shear Modulus GV
35 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
47 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
50 GPa
Elastic Anisotropy
0.90
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YbClF (mp-557483) 0.1409 0.000 3
KMnBi (mp-1018739) 0.1389 0.233 3
KMgP (mp-1018737) 0.1430 0.000 3
KMnSb (mp-4233) 0.0720 0.147 3
SrBrF (mp-23024) 0.0510 0.000 3
Na2LiAlP2 (mp-9719) 0.5645 0.000 4
K2LiGaAs2 (mp-9703) 0.4884 0.000 4
K2NaInP2 (mp-21511) 0.5733 0.000 4
K2NaInAs2 (mp-21510) 0.5772 0.000 4
K2LiInAs2 (mp-505431) 0.4252 0.000 4
SrAl2 (mp-1071777) 0.4124 0.013 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Fe_pv As
Final Energy/Atom
-5.0959 eV
Corrected Energy
-30.5754 eV
-30.5754 eV = -30.5754 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 163144
  • 163143
Submitted by
User remarks:
  • Sodium iron arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)